Metric Extruded Aluminium Channel
Product Description
Nws yog lub npe hu ua architectural aluminium channel, feem ntau siv thiab txais kev lag luam hauv kev lag luam, tsim khoom thiab kev tsim kho raws li nws qhov zoo malleability.All aluminium extrusion channel duab muaj nyob rau hauv zeb tiav, ntshiab anodized, dub anodized, kub anodized, thiab pleev xim rau. Muaj ntau txoj hauv kev hauv ntau cov duab thiab ntau thiab tsawg, nws muaj kev xaiv ua tiav ntawm cov qauv tsim, tees.Peb muaj kev txawj ntse hauv kev tsim thiab fabrication, uas txhais tau hais tias peb tuaj yeem txaus siab rau txhua daim ntawv thov thiab peb cov khoom yuav tshaj qhov koj xav tau.
Khoom Taw Qhia
Tshuaj muaj pes tsawg leeg ntawm Aluminium Extrusion Profiles | |||||
Alloy | 6063 | 6061 | 6060 | 6005 | |
Si | 0.2-0.6 | 0.4-0.8 | 0-0.6 | 0-0.9 | |
Mg | 0.45-0.9 | 0.8-1.2 | 0.35-0.6 | 0.4-0.6 | |
Fe | <0.35 | <0.7 | 0.1-0.3 | 0.35 | |
Cu | <0.1 | 0.15-0.4 | Tsawg dua lossis sib npaug rau 0.1 | 0.1 | |
Mn | <0.1 | <0.15 | Tsawg dua lossis sib npaug rau 0.1 | 0.1 | |
Zn | <0.1 | <0.25 | Tsawg dua los yog sib npaug rau 0.15 | 0.1 | |
Cr | <0.1 | 0.04-0.35 | Tsawg dua lossis sib npaug rau 0.05 | 0.1 | |
Ti | <0.1 | <0.15 | <0.1 | 0.1 | |
impurity | Chav tsev | <0.05 | <0.05 | <0.05 | <0.05 |
Tag nrho | <0.15 | <0.15 | <0.15 | <0.15 | |
Al | Tseem tshuav | Tseem tshuav | Tseem tshuav | Tseem tshuav | |
Technical Data ntawm Aluminium Extrusion Profiles | ||||||
Alloy | Kub | Thickness | Tensile | Yield | Vickers | Webster |
Lub zog | Lub zog | Hardness | Hardness | |||
6005 | T6 | Tsawg dua los yog sib npaug li 5 | Ntau dua lossis sib npaug li 270MP | Ntau dua lossis sib npaug li 225MP |
|
|
T6 | 5<e Tsawg dua lossis sib npaug li 10 | Ntau dua lossis sib npaug li 260MP | Ntau dua lossis sib npaug li 215MP |
|
| |
T6 | 10<e Tsawg dua lossis sib npaug li 25 | Ntau dua lossis sib npaug li 250MP | Ntau dua lossis sib npaug li 200MP |
|
| |
6060 | T6 | Tsawg dua los yog sib npaug 3 | Ntau dua lossis sib npaug li 190MP | Ntau dua lossis sib npaug li 150MP |
|
|
T6 | 3<e Tsawg dua lossis sib npaug li 25 | Ntau dua lossis sib npaug li 170MP | Ntau dua lossis sib npaug li 140MP |
|
| |
6061 | T6 |
| Ntau dua lossis sib npaug li 265MP | Ntau dua lossis sib npaug li 245MP | HV Ntau dua lossis sib npaug rau 58 | HW Ntau dua lossis sib npaug rau 8 |
6063 | T5 |
| Ntau dua lossis sib npaug li 160MP | Ntau dua lossis sib npaug li 110MP | HV Ntau dua lossis sib npaug rau 58 | HW Ntau dua lossis sib npaug rau 8 |
T6 |
| Ntau dua lossis sib npaug li 205MP | Ntau dua lossis sib npaug li 180MP | HV Ntau dua lossis sib npaug rau 58 | HW Ntau dua lossis sib npaug rau 8 | |
Nta
◆ Ua haujlwm tau:Nws muaj kev lees paub zoo ntawm cov txheej txheej xws li anodized lossis pleev xim tiav.6063 raws yog yooj yim rau vuam, thiab kuj yog mos thiab yooj yim rau txiav.
◆ Zoo zoo raw khoom:6063 alloy muaj kev lees paub zoo ntawm cov txheej txheem siv xws li anodized lossis pleev xim tiav. 6063 raws yog yooj yim rau weld, thiab kuj yog mos thiab yooj yim rau txiav.6063 alloy yuav machined, tab sis tsis tshuab raws li ib tug nyuaj alloys zoo li 6061.
◆ Anodizing:Nws yog cov txheej txheem tshuaj uas ua kom nrawm thiab ua kom cov txheej txheem tiv thaiv oxide tshwm sim.No chipping, tsis flaking, tsis tev.
◆ Tshuab tiav:Rau lub hom phiaj ntawm kev tshem tawm me me imperfections thiab tsim kom muaj lustrous tiav.
Sectional Drawing

Khoom Saib

Ntim
FAQ
Q1.Dab tsi yog koj qhov kev txiav txim siab ntev npaum li cas thiab kuv tuaj yeem hais qhia qhov kev zam tshwj xeeb?
A: Peb tus qauv kam rau ua rau qhov ntev txiav yog "±.003". Yog tias koj xav tau kev zam tshwj xeeb, thov nco ntsoov qhov no ntawm qhov kev txiav txim hauv cov ntawv sau lossis hauv "qhov tshwj xeeb txiav ntev" teb.
Q2.Nws yuav siv sijhawm ntev npaum li cas los xa?
A: 10-20 hnub ib txwm.
Q3.Dab tsi txog qhov zoo?Puas yog txhuas channel raws li European qauv?
A: Kev tshuaj xyuas tus kheej yuav ua tiav ua ntej shipping.Thiab peb cov khoom yuav ua tau raws li cov qauv hauv zos.
Q4.Apart from standard aluminium extrusion ntau lawm, ua li cas txog kev cai dimension?
A: Cov khoom lag luam tau txais tos zoo heev.Yog tias peb tsis muaj cov extruded aluminium channel uas ua tau raws li qhov yuav tsum tau ua, peb cov kws tshaj lij yuav pab koj nrog engineering. Peb lav tias peb tuaj yeem tsim cov aluminium channel duab uas ua tau raws li koj qhov loj me specifications.
Cim npe nrov: metric extruded aluminium channel, Tuam Tshoj, tuam ntxhab, lwm tus muag khoom, Hoobkas, customized, lag luam wholesale, nqe, kev muag khoom
Koj Tseem Yuav Zoo Li
Xa kev nug