Cov Kev Ntsuas (Parameter)

Cov khoom

6000 series Aluminium Alloy

Temper

T5, T6

Qhov Coob / Thickness

Profile thickness: 0.8 rau 5.0 hli
Anodize zaj duab xis thickness: 10 ~ 20 um
Ntev: ≤7000mm / customized muaj

Fabrication Txheej Txheem

Kev Tiv Thaiv, Kev Kub Ntxhua (High Speed), Tapping, Precise Txiav, Milling (CNC)

Daim ntawv thov

Rau tshav kub kub rau lub cav tsheb thaub ntiag tug
Rau tshav kub kub rau Cov teeb pom kev zoo, teeb pom kev zoo LED txoj kev teeb pom kev zoo, theem teeb pom kev zoo, LED qhov teeb pom kev zoo thiab lwm yam


Cov Lus Qhia Taw Qhia

Aluminium Cov Tshuaj Txhaum Cov Tshuaj

Alloy

6063 (%)

6061 (%)

Si

0.2-0.60

0.4-0.8

Fe

0.35

0.70

Cu

0.10

0.150-.40

Mn

0.10

0.15

Mg

0.45-0.90

0.80-1.20

Cr

0.10

0.04-0.35

Zn

0.10

0.25

Ti

0.10

0.15

Al

Ncua tseg

Ncua tseg

Tensile zog

σ b (Mpa): ≥ 250

(MPa): ≥180

Elongation kev ntxhov siab

σ p0.2 (Mpa): ≥ 110

σ p0.2 (Mpa): ≥ 110

Kev loj hlob

δ 5 (%): ≥ 7

δ5 (%): ≥ 14

Aluminium 6063-T5, k = 201 W / mK (tshaj plaws)

Aluminium 6061-T5, k = 167 W / mK


Cov lus qhia

Yam khoom

Seem

Cov khoom

Qhov siab (hli)

Dav (hli)

Thykkness (hli)

Thaj Chaw (mm²)

Qhov hnyav (kg / m)

H06001

image002

6063-T5

24 ± 0.2

60 ± 0.2

1.9

416.4

1.12

H06002

image004

6063-T5

23.3 ± 0.2

117

3.8 ± 0.2

625.61

1.71

H06003

image006

6063-T5

23.3 ± 0.2

94 ± 0.2

3.8 ± 0.2

626.45

1.71

W77001

image008

6063-T5

45

95

4.5

1267

3.45


Khoom Zaub

image010image012image014


Ntim thiab Xaib

image016image018image020


Cov txiaj ntsig

Turnkey extrusions thiab fabrication

Los ntawm CAD thiab prototyping mus sib dhos thiab xaib, peb extrusion thiab fabrication cov kev pab cuam nrog peb ntau yam ntawm cov qauv siv, engineering, machining thiab kauj xauv daws, muab koj txhua yam koj xav tau nyob rau hauv ib lub ru tsev.


Bespoke daws

Tsis muaj ib tus neeg twg-haum-txhua txoj kev los ntawm YIDA lub tuam txhab Peb paub tias txhua lub lag luam txawv, thiab peb mloog koj xav tau dab tsi thiab txheeb peb txoj kev ua kom haum koj. Ua hauj lwm zoo nrog peb lub ntiaj teb no network ntawm ntseeg koom tes, peb muaj qhov yooj yooj yim los nrhiav koj lub zoo meej daws.

Cim npe nrov: aluminium extruded dab dej kub, Suav teb, manufacturers, lwm tus neeg, Hoobkas, customized, lag luam wholesale, nqe, kev muag khoom

Xa kev nug

whatsapp

Xov tooj

Tug

Kev nug