Extruded Aluminium Kub Sov
Cov Lus Qhia Khoom
Nws yog txoj kev daws teeb meem zoo tshaj plaws los ua kom lub cev kub hnyav ua rau nws lub cev, nws qhov sib tw, kev thermal conductivity thiab hnav. Nws yog ib puag ncig tus phooj ywg thiab muaj peev xwm txais kev kawm zoo tshaj plaws.Thiab ua yooj yim, xws li kev kho tiav txhua yam, kev kho mob thiab kev kho siab , Anti-corrosion muaj peev xwm thiab muab kev cai tsim.Specifically, 'YIDA' lub tuam txhab muab CNC machining rau converting fins ntawm extruded tshav kub dab rau hauv pins.Qhov feem ntau aluminium yog 6063-T5, tab sis lwm 6000 series alloys tseem yuav kuaj yog xav tau.
Cov Lus Qhia Taw Qhia
Aluminium Cov Tshuaj Txhaum Cov Tshuaj | ||
Alloy | 6063 (%) | 6061 (%) |
Si | 0.2-0.60 | 0.4-0.8 |
Fe | 0.35 | 0.70 |
Cu | 0.10 | 0.150-.40 |
Mn | 0.10 | 0.15 |
Mg | 0.45-0.90 | 0.80-1.20 |
Cr | 0.10 | 0.04-0.35 |
Zn | 0.10 | 0.25 |
Ti | 0.10 | 0.15 |
Al | Ncua tseg | Ncua tseg |
Tensile zog | σ b (Mpa): ≥ 250 | (MPa): ≥180 |
Elongation kev ntxhov siab | σ p0.2 (Mpa): ≥ 110 | σ p0.2 (Mpa): ≥ 110 |
Kev loj hlob | δ 5 (%): ≥ 7 | δ5 (%): ≥ 14 |
◆ Aluminium 6063-T5, k = 201 W / mK (tshaj plaws)
◆ Aluminium 6061-T5, k = 167 W / mK
Cov lus qhia
Yam khoom | Seem | Cov khoom | Qhov siab (hli) | Dav (hli) | Thickness (hli) | Thaj Chaw (hli ² ) | Qhov hnyav (kg / m) |
H06001 | ![]() | 6063-T5 | 24 ± 0.2 | 60 ± 0.2 | 1.9 | 416.4 | 1.12 |
H06002 |
| 6063-T5 | 23.3 ± 0.2 | 117 | 3.8 ± 0.2 | 625.61 | 1.71 |
H06003 | ![]() | 6063-T5 | 23.3 ± 0.2 | 94 ± 0.2 | 3.8 ± 0.2 | 626.45 | 1.71 |
W77001 |
| 6063-T5 | 45 | 95 | 4.5 | 1267 | 3.45 |
Khoom zaub
Daim ntawv pov thawj
Lus nug
Q1. Dab tsi yog koj tus qauv txiav kev kam rau siab ntev thiab kuv tuaj yeem qhia meej tau ib qhov kev siab ntev?
A: Peb txheem kam rau sab ntev yog '± .003'. Yog tias koj xav tau kev zam rau tshwj xeeb, thov nco ntsoov qhov no ntawm qhov kev txiav txim los ntawm cov lus sau los yog hauv qhov "specific cut length".
Q2.What txog ntau lub thickness tsim thaum lub sij hawm ntau lawm?
A: Aluminium yuav tau buffed, blasted, polished, grinded los yog sanded.These finishes yuav ua kom zoo zoo.
Q3.Kuv ntev npaum li cas nws yuav coj mus rau?
A: 10-20days rau cov uas twb muaj lawm mould.Custom product xav tau sij hawm ntxiv rau tus me nyuam. Thov tuaj yeem tiv tauj peb.