Extruded aluminium t slot yog ib qho yooj yim tov rau connectors, fasteners thiab accessories.Thaum koj ces yuav tsum nyob rau hauv lub inconvenience ntawm tsiv thiab positioning hnyav pieces ntawm hlau, drilling, tapping, series ntawm ntau lawm dab annoying koj.Yog li tej yees ntawm aluminium ntau lawm, tam sim no T-slot txhuas muaj tshwm sim thiab yuav yog ib qho kev xaiv kom zoo saib yog tias koj tab tom nrhiav cov khoom siv hluav taws xob thiab ua kom ntev.


Cov Kev Ntsuas (Parameter)

Tshuaj Txhaum Tshuaj Txhuas Txhuas Txhuas Extrusion Profiles

Alloy

6063

6061

6060

6005

Si

0.2-0.6

0.4-0.8

0-0.6

0-0.9

Mg

0.45-0.9

0.8-1.2

0.35-0.6

0.4-0.6

Fe

<>

<>

0.1-0.3

0.35

Cu

<>

0.15-0.4

≤0.1

0.1

Mn

<>

<>

≤0.1

0.1

Zn

<>

<>

≤0.15

0.1

Cr

<>

0.04-0.35

≤0.05

0.1

Ti

<>

<>

<>

0.1

Kev qias neeg

Chav tsev

<>

<>

<>

<>

Tag nrho

<>

<>

<>

<>

Al

Ncua tseg

Ncua tseg

Ncua tseg

Ncua tseg


Cov ntaub ntawv ntawm Aluminium Extrusion Profiles

Alloy

Temper

Thickness

Tensile

Tawm

Vickers

Webster

Zog

Zog

Hardness

Hardness

6005

T6

≤5

≥270MP

≥225MP

T6

5 <>

≥260MP

≥215MP

T6

10 <>

≥250MP

≥200MP

6060

T6

≤3

≥190MP

≥150MP

T6

3 <>

≥170MP

≥140MP

6061

T6

≥265MP

≥245MP

HV58

HW = 8

6063

T5

≥160MP

≥110MP

HV58

HW = 8

T6

≥205MP

≥180MP

HV58

HW = 8


Seem duab seem

image003


Nta

◆ Xws li ruaj khov.Thaum nws possesses lub zog-rau-phaus piv uas ua tau zoo tshaj ntawm cov hlau.

◆ Durability.It cov ntaub ntawv tiv thaiv fawm thaum nws tawm mus rau hauv oxidation.Tsis yuav tsum tau prime thiab xim

◆ Precision hauv fabrication.Li dimension yuav customized.

◆ Zoo adaptation.Puas khoom yog zoo-txawm peem rau nrog cov khoom phiaj.

1


Pwm thiab Kho Mob

2


Lus nug

Q1. Hom kev pab cuam rau cov khoom txeem extruded?

A: Peb muaj ob peb lub tshuab CNC uas yog siv los kho cov khoom siv hluav taws xob rau hauv qhov cub ua kom sov dua hauv qhov pins.Dab tsi ntau, drilling, ntsej muag milling, tapping kuj muaj.


Q2.What txog ntau lub thickness tsim thaum lub sij hawm ntau lawm?

A: Aluminium yuav tau buffed, blasted, polished, grinded los yog sanded.These finishes yuav ua kom zoo zoo.


Q3.What txog kev them nqi?

A: 30% rau kev tso nyiaj, tshuav nqi ua ntej tus me nyuam.

Cim npe nrov: extruded aluminium t slot, Suav teb, manufacturers, lwm tus neeg, Hoobkas, customized, lag luam wholesale, nqe, kev muag khoom

Xa kev nug

whatsapp

Xov tooj

Tug

Kev nug