Aluminium Extrusion SCRIPTION SCRapping raws li lub tuam txhab ntawm cov khoom siv tswj hwm, ua tib zoo ua haujlwm ntawm kev siv pwm, thiab kom ntau lawm, cov qauv no tshwj xeeb.
Muaj ntau cov laj thawj rau cov ntxiab ntawm txhuas pwm: Ua ntej ntawm txhua yam, cov haujlwm ua haujlwm ntawm txhuas exsh, thiab lawv raug coj los ua kom nruj thiab kev coj ua kom sov thiab siab.
(1) Kev sib txhuam thiab cov ris tsho ua haujlwm rau 65%,
(2) Qeeb Qeeb Qeeb Ua Haujlwm Nyiaj Txiag rau 18%,
(3) Yas deformation thiab ua tiav cov nyiaj tsis tiav rau 15%. Kev txiav txim siab ntawm kev ua tsis tau los ntawm cov pwm tsis ua tiav yog raws cov khoom lag luam uas tsis tuaj yeem ua tau, thiab cov kev pabcuam lub neej tau raug piav qhia los ntawm kev siv hluav taws xob zoo.
1. Scrapping txheej txheem thaum cov pwm pom tau ua puas lossis hnav tau los ntawm cov neeg tsim khoom lag luam scrapping, uas tau txais kev pom zoo los ntawm tus thawj tswj hwm ntawm lub tuam txhab. Thiab cov tswv yim qhia txuj ci siv los ua ntxiv ntxiv
2. Scrapping Cov Qauv Txheej Txheem rau Pwm Scrapping Kev Cai thiab cov txheej txheem kev tswj hwm cov cuab tam los ntawm cov tuam txhab, uas tau hais raws li hauv qab no:
Cov Txheej Txheem Qhia Ua Zoo Rau Cov Ntsuam Xyuas
(1) Thaum cov khoom tau nres tau txais cov ntawv xaj thiab cov khoom tsim los ntawm cov pwm yog qhov chaw siv.
(2) Thaum lub neej pabcuam ntawm cov pwm tau xaus, thiab nws tau raug puas tiag tiag thiab tsis tuaj yeem kho thiab siv.
(3) Vim tsim kev hloov pauv, cov khoom qub raug hloov pauv, thiab pwm tsis tuaj yeem hloov lossis siv rau lwm lub hom phiaj.
(4) Cov pwm cov pwm tawg, thiab qhov chaw ntawm cov khoom uas yuav tsum tau ua raws li cov khoom yuav tsum tau ua;
(5) Tus lej ntawm cov pwm txheem yog qhov siab, thiab nws tsis yog lawm tom qab ntau tshaj 3 zaug ntawm "kev sib tham sib tham";
(6) Cov pwm yog welded hauv ntau qhov chaw, feem ntau puas, thiab tsis tuaj yeem ua tiav ntawm ib qho hloov pauv ib txwm;
(7) Cov ntxig loj ntawm cov pwm raug tawg, thiab cov remanufacture ntawm cov ntxig tsis muaj nyiaj txiag;
(8) Vim yog tsim qauv thiab tsim khoom lag luam, pwm feem ntau lo rau pwm, qhov loj tshaj, thiab tsawg dua
(9) Thaum lwm yam ua rau cov pwm kom tsis muaj kev siv tus nqi