Sep 16, 2025 Tso lus

Kev tsom xam ntawm cov laj thawj rau tsis - Ua raws li cov khoom siv cov kho tshuab ntawm txhuas cov txheej txheem thiab cov kev daws teeb meem

Analysis of the reasons for non-compliance of mechanical properties of aluminum profiles and solutions

Qhov laj thawj tseem ceeb:
 

(1) qhov ntsuas kub tsawg dhau thaum lub sijhawm extrusion ntawm aluminium profiles, thiab cov extruden ceev yog qeeb, uas tsis tau txais kev daws teeb meem zoo;

 

(2) Tsis muaj cov kiv cua tsis txaus ntawm qhov profile tawm, ua rau cov cua txias dua, ua rau cov khoom siv couring ntau dua, ua rau cov neeg siv tshuab ntawm cov profile ntawm kev kho cua sov;

 

(3) Cov lej sib xyaw ua ke tsis tsim nyog, thiab cov ntsiab lus mg thiab Si cov ntsiab lus hauv Ingot tsis tau raws li cov qauv yuav tsum tau ua;

 

(4) Cov kev ua haujlwm sib xyaw tsis yog homogenization kev kho mob, ua rau lub sijhawm mg2si precipitated nyob rau hauv lub sij hawm ingot

 

(5) Kev laus tsis raug cai, lossis cov cua tsis zoo cua, lossis tsis yog thermocouple installation txoj hauj lwm ua rau tsis muaj kev laus lossis tshaj {1}-}-

 

Kev daws:

 

(1) Tsim nyog tswj qhov kev tshem tawm kub thiab nrawm kom ua kom cov profile tawm ntawm qhov ntsuas kub ntawm qhov tsawg kawg nkaus cov kua kub;

 

(2) ntxiv dag zog rau cov huab cua txias, thiab cov chaw ua haujlwm tuaj yeem txhim kho atomizing txias cov khoom siv rau 6063 alloy;

 

(3) ntxiv dag zog rau kev tswj hwm zoo ntawm kev cuam tshuam;

 

(4) ua homogenogenization ntawm kev ua;

 

(5) Tsim kev txiav txim siab cov kev laus, kho cov thermocouples, thiab muab cov profile kom huv si kom ntseeg tau tias cov cua sov huab cua. Geometric qhov ntev tshaj kev kam kam.

Xa kev nug