Txij li thaum tus yam ntxwv tseem ceeb ntawm 6082 aluminium alloy yog nws cov ntsiab lus ntawm cov hlau refractory Mn, qhov tsim nyog muaj Mn tuaj yeem ua rau muaj kev sib cais ntawm intracranular thiab txo cov plasticity hauv cov khoom hauv cov khoom -kua cheeb tsam, ua rau tsis muaj kev sib tsoo tsis txaus. Yog li ntawd, cov txheej txheem casting feem ntau yuav tsum tau tsom mus rau peb lub ntsiab lus: Ua ntej, thaum lub sij hawm melting, yuav tsum tau them nyiaj rau kev tswj qhov kub thiab txias ntawm 740 ~ 760℃thiab nplawm kom huv si kom tiav cov hlau melting, qhov kub thiab txias, thiab cov khoom muaj pes tsawg leeg. Qhov thib ob, thaum lub sij hawm casting, nws yuav tsum tau txiav txim siab hais tias lub xub ntiag ntawm Mn tsub kom lub alloy lub viscosity, txo nws fluidity thiab cuam tshuam rau cov alloy qhov kev ua tau zoo. Lub casting ceev yuav tsum tau txo kom zoo thiab tswj nyob rau hauv qhov ntau ntawm 80 ~ 100 mm / min. Thib peb, ua kom qhov txias txias thiab ua kom lub zog txias ntawm cov txhuas profiles los pab tshem tawm cov kev sib cais ntawm cov intragranular. Tswj thawj qhov kev siv txias txias thiab ua kom cov cua txias thib ob kom txo qis kev ntxhov siab thaum lub sij hawm casting thiab tsis txhob ingot cracking defects. Cov dej txias siab yuav tsum tau tswj nyob rau hauv thaj tsam ntawm 0.1 ~ 0.3 MPa.
Ua rau thiab cov kev daws teeb meem rau Aluminium Profile ua tsis tiav xim:
1. Anodic oxide zaj duab xis yog nyias heev. Qhov kev daws teeb meem yog los xyuas seb cov txheej txheem anodizing puas yog tus qauv, thiab seb yam xws li qhov kub thiab txias, qhov hluav taws xob, thiab conductivity puas ruaj khov. Yog tias pom qhov txawv txav, kho kom haum raws li cov qauv. Yog tias tsis muaj qhov txawv txav, lub sijhawm oxidation tuaj yeem tsim nyog txuas ntxiv kom ntseeg tau tias cov yeeb yaj kiab tuab ua tau raws li qhov yuav tsum tau ua.
2. Tus nqi pH ntawm cov tshuaj dye yog siab dhau. Hauv qhov no, acetic acid ice tuaj yeem siv los kho cov pH rau tus nqi tus qauv.
3. Lub oxidized workpiece tau tso rau hauv lub tank dej ntev dhau lawm. Nws raug nquahu kom dye lub workpiece kom sai. Yog tias qhov no tau tshwm sim lawm, cov khoom ua haujlwm tuaj yeem tsim nyog rov ua haujlwm hauv lub tank anodizing lossis nitric acid neutralization tank ua ntej dyeing, ua rau muaj txiaj ntsig zoo.
4. Cov xim xaiv tsis tsim nyog. Cov xim zoo nkauj yuav tsum tau xaiv.
5. Cov xim tau decomposed los yog molded. Hauv qhov no, cov xim yuav tsum tau hloov.
6. Oxidation kub tsawg dhau, ua rau cov yeeb yaj kiab ntom ntom. Qhov kub oxidation tuaj yeem nce nruab nrab.
7. Tsis zoo conductivity. Qhov no tej zaum yuav yog vim kev sib cuag tsis zoo nyob rau hauv anodic tooj liab pas nrig los yog cathodic txhuas phaj, uas ua rau tsis zoo batch conductivity.
Ua tib zoo saib xyuas cov anode tooj liab rods thiab cathode txhuas daim hlau kom ntseeg tau tias muaj kev ua tau zoo.
Vim hais tias cov pwm rau radiator profiles muaj ntau nyias, elongated cov hniav uas yuav tsum tau tiv taus siab extrusion siab, txhua tus hniav yuav tsum muaj siab zog thiab toughness. Yog tias muaj qhov sib txawv tseem ceeb hauv kev ua haujlwm ntawm cov hniav, cov neeg uas muaj zog qis lossis tawv tuaj yeem tawg tau yooj yim. Yog li ntawd, qhov zoo ntawm cov pwm hlau yuav tsum txhim khu kev qha. Nws yog qhov zoo tshaj plaws los siv H13 steel uas tsim los ntawm cov tuam txhab muaj koob npe lossis siab -cov hlau zoo. Kev kho cua sov ntawm pwm yog qhov tseem ceeb heev; Lub tshuab nqus tsev cua sov thiab quenching yuav tsum tau siv, nrog siab - siab ntshiab nitrogen quenching yog qhov kev xaiv zoo tshaj plaws, vim nws ua kom cov khoom sib xws thoob plaws txhua qhov ntawm cov pwm tom qab quenching. Tom qab quenching, peb txheej txheem tempering yuav tsum tau ua los xyuas kom meej tias cov pwm hardness yog tswj ntawm HRC48-52 thaum muab txaus toughness. Qhov no yog ib qho teeb meem tseem ceeb los tiv thaiv pwm cov hniav los ntawm kev tawg.