Cov xim electrolytic ntawm aluminium profiles muaj cov khoom zoo nkauj zoo nkauj, thiab yog li nws tau siv dav hauv ob qho tib si hauv tsev thiab txawv teb chaws, tshwj xeeb tshaj yog nyob rau hauv kev kho deg ntawm cov vaj tse aluminium profiles. Tam sim no, cov txheej txheem tseem ceeb siv lub tin -nickel tov ntsev electrolytic xim txoj kev, nrog rau cov khoom feem ntau nthuav tawm xim champagne. Piv rau ib qho xim nickel ntsev xim, cov khoom tsim nrog tin -nickel tov ntsev electrolytic xim muaj xim ci thiab tag nrho cov tones. Qhov teeb meem tseem ceeb yog tias cov khoom yuav muaj xim sib txawv, uas tuaj yeem tshwm sim los ntawm cov txheej txheem extrusion tsis tsim nyog thiab cov txheej txheem xim anodizing thaum lub sij hawm txhuas profile ntau lawm.
Kev cuam tshuam ntawm cov txheej txheem extrusion ntawm anodizing xim feem ntau yog yuav ua li cas pwm tsim, extrusion kub, extrusion ceev, thiab txias txoj kev cuam tshuam rau saum npoo thiab uniformity ntawm extruded profiles. Kev tsim pwm yuav tsum cia cov khoom sib xyaw kom txaus; txwv tsis pub, qhov tsis xws luag xws li ci (lossis tsaus nti) bands yuav tshwm sim, thiab xim txawv yuav tshwm sim ntawm tib qhov profile. Tsis tas li ntawd, cov pwm mob thiab cov cim extrusion ntawm qhov profile nto kuj cuam tshuam rau cov xim anodizing. Qhov sib txawv ntawm extrusion kub, ceev, txias txoj kev, thiab lub sij hawm txias tuaj yeem ua rau cov qauv tsis sib xws.
1. Nws kuj tuaj yeem ua rau muaj xim txawv.
Anodizing muaj qhov cuam tshuam loj rau cov xim sib txawv hauv cov xim electrolytic, tshwj xeeb tshaj yog nyob rau hauv cov txheej txheem ntawm cov kab ntsug anodizing, qhov twg xim sib txawv ntawm ob qhov kawg yog qhov tshwm sim. Vertical anodizing tso tsheb hlau luam yog 7.5 meters sib sib zog nqus, thiab kub sib txawv yooj yim tsim ntawm sab saum toj thiab hauv qab ntawm lub tso tsheb hlau luam. Kub muaj qhov cuam tshuam tseem ceeb ntawm anodizing; Qhov kub thiab txias dua ua kom qhov sib xyaw ntawm cov oxide zaj duab xis nyob rau hauv cov tshuaj anodizing, ua rau cov pore loj nyob rau saum npoo ntawm cov ntxeem tau anodic oxide zaj duab xis, qhov kub qis ua rau cov pores me me. Tsis tas li ntawd, qhov kub siab dua ua rau cov porosity ntau dua ntawm anodic oxide zaj duab xis, thiab qhov kub thiab txias ua rau qis porosity.
Electrolytic colouring feem ntau ua haujlwm los ntawm kev ua rau cov hlau ions hauv cov xim pleev xim kom tau txais cov tshuaj tiv thaiv electrochemical txo rau ntawm qhov chaw thaiv txheej hauv micropores ntawm oxide zaj duab xis. Qhov no ua rau lub deposition ntawm hlau ions nyob rau hauv qab ntawm lub pores nyob rau hauv lub anodic oxide zaj duab xis, scattering teeb meem teeb meem thiab tsim cov xim sib txawv. Qhov ntau cov khoom tso rau hauv micropores, qhov tob xim. Nyob rau hauv cov xwm txheej ntawm tib cov ntaub ntawv tam sim no, tib cov nqi ntawm cov hlau los yog cov hlau sib txuas yuav tso rau hauv qhov chaw siab thiab qis, tab sis nyob rau hauv cov cheeb tsam uas muaj qhov porosity siab thiab qhov pores loj dua, txhua qhov pore yuav tau txais nyiaj tsawg dua, ua rau cov xim sib dua, thaum cov xim yuav tsaus dua nyob rau hauv cov cheeb tsam uas tsis muaj porosity thiab me pores. Qhov no ua rau muaj xim txawv ntawm ob qhov kawg ntawm cov khoom. Thaum lub sij hawm anodizing, conductivity kuj cuam tshuam rau oxide zaj duab xis thiab tuaj yeem ua rau xim sib txawv. Qhov teeb meem no muaj ntau dua nyob rau hauv kab rov tav ntau lawm, feem ntau vim hais tias thaum lub sij hawm ua ntej - anodizing teeb, yog tias cov clamps tsis nruj, qee cov ntaub ntawv ua haujlwm tsis zoo, ua rau muaj qhov sib txawv ntawm cov yeeb yaj kiab anodic. Tom qab coloring, qhov no ua rau cov xim txawv.
Cov txheej txheem xim electrolytic tuaj yeem qhia ncaj qha rau cov teeb meem xim txawv. Lub peev xwm ntawm cov tshuaj pleev xim rau kev faib tawm tam sim no plays lub luag haujlwm txiav txim siab kom ua tiav cov xim sib xws. Kev faib tsis sib xws tam sim no ua rau pom cov xim sib txawv. Qhov kev daws teeb meem tam sim no muaj peev xwm faib tau feem ntau cuam tshuam nrog cov conductivity thiab polarization ntawm cov tshuaj. Cov tshuaj pleev xim muaj qee cov ntsev conductive los txhim kho conductivity. Yog tias cov ntsev zoo li no tsis tau ntxiv rau lub sijhawm, conductivity txo, txo cov peev txheej tam sim no thiab ua rau muaj xim sib txawv. Tsis tas li ntawd, cov additives hauv cov tshuaj pleev xim tuaj yeem muaj cov khoom adsorption tshwj xeeb, nce polarization. Kev noj ntau dhau ntawm cov tshuaj no txo cov polarization ntawm electrolyte, txo cov peev txheej tam sim no, thiab ua rau muaj xim txawv. Hauv kev tsim khoom tiag tiag, nws yog ib qho tsim nyog tsis yog txhawm rau txhim kho cov conductivity ntawm cov tshuaj, tab sis kuj yuav tsum xyuas kom meej tias cov pas nrig conductive thiab tooj liab muaj qhov zoo conductivity. Kev ua haujlwm tsis zoo ua rau cov kab hluav taws xob tsis sib xws, ua rau muaj xim sib txawv.
Lub hom phiaj tseem ceeb yog nyob ntawm ntau yam uas ua rau muaj xim sib txawv hauv tib batch ntawm cov khoom. Kev hloov pauv hauv cov txheej txheem tsis muaj anodizing thiab xim electrolytic tuaj yeem ua rau cov xim sib txawv ntawm cov khoom sib txawv. Yog li ntawd, hauv kev tsim khoom, nws yog ib qho tsim nyog los tswj kev ruaj ntseg ntawm cov txheej txheem oxidation thiab xim thiab ua kom zoo ib yam ntawm txhua qhov tsis sib xws, yog li txo qhov tshwm sim ntawm cov xim sib txawv ntawm cov khoom siv oxidized thiab xim.