Xaiv dyes rau aluminium anodizing khoom

1. Xaiv Dyes rau Aluminium Oxidation Equipment

 

Muaj ntau ntau hom organic dyes, thiab qhov kev xaiv nyob ntawm qhov kev npaj siv thiab qib khoom. Soluble reactive dyes yog kim tab sis muaj cov xim zoo heev, yog li lawv feem ntau siv los zas cov khoom siv high-end aluminium xws li cwj mem, teeb, thiab cov khoom siv hnov ​​lus. Cawv-soluble dyes yog siv rau cov xim txhuas ntawv ci, thaum cov roj-soluble dyes yog siv rau txhuas ntawv nyiaj luam ntawv. Ua ntej siv, roj-soluble dyes yog yaj nyob rau hauv nitrocellulose-raws li, ethylene-resin-based, los yog polyamide-resin-raws li varnishes, los yog nyob rau hauv melamine thiab epoxy resins nyob rau hauv ci xim. Tom qab luam ntawv, lawv tsim ib zaj duab xis resin uas muaj cov zas xim rau ntawm cov ntaub ntawv uas huv si. Cov hom dyes siv rau cov xim txhuas cov khoom muaj xws li acid dyes, acid complex dyes, acid mordant dyes, ncaj dyes, me acid dyes, disperse dyes, soluble reactive dyes, reactive dyes, yooj yim dyes, cawv-soluble dyes, roj-soluble dyes, thiab ntau dua.

 

2. Anodized Aluminium Equipment Organic Dye Coloring txheej txheem thiab tswj

 

Ib leeg-xim dyeing: Tom qab anodizing aluminium cov khoom thiab yaug lawv nrog dej huv, muab tso rau hauv cov xim da dej ntawm qhov ntsuas kub. Lub sij hawm dyeing nyob ntawm qhov tob xim, thiab da dej ntim tuaj yeem tswj tau ntawm 10: 1 piv piv rau qhov ntim ntawm cov khoom.

 

Ntau xim dyeing: Yog tias dyeing txhuas qhov chaw nrog ob lossis ntau xim sib txawv, xws li toj roob hauv pes, paj thiab noog, cov qauv, lossis cov ntawv nyeem, cov txheej txheem luam ntawv feem ntau yog siv. Cov ntawv luam tawm tuaj yeem yog daim phiaj nyem (zinc lossis ntawv) lossis cov ntawv lo lo ntxhuav, thiab cov txheej txheem yuav suav nrog kev luam ntawv ncaj qha, tiv thaiv txheej, lossis ua npuas dej. Feem ntau, cov txheej txheem suav nrog kev dyeing thawj xim, siv cov txheej txheem tiv thaiv rau cov cheeb tsam uas txhais tau tias khaws cov xim ntawd, tshem cov xim seem, thiab rov ua cov txheej txheem thib ob, thib peb, thiab lwm yam xim ntxiv.

Xa kev nug

whatsapp

Xov tooj

Tug

Kev nug