5. Poob gloss ntawm cov txheej txheej
Ua rau:
1. Tsis zoo pretreatment zoo ntawm lub substrate.
2. Ci lub sij hawm ntev los yog kub heev.
3. Cov pa hluav taws xob muaj nyob hauv qhov cub.
4. Kev siv cov hmoov nplej ntau dhau.
5. Kev sib xyaw ntawm ob lub hmoov uas muaj cov khoom sib txawv.
6. Cov hmoov txheej tsis zoo.
Kev daws:
1. Xaiv cov txheej txheem ua ntej kom tsim nyog.
2. Kho cov kev kho kom haum.
3. Ntxuav lub qhov cub.
4. Lim cov hmoov siv ua ntej sib xyaw nrog cov hmoov tshiab, ua kom nws qis dua 30%.
5. Ua tib zoo ntxuav cov hmoov txau ua ntej hloov cov hmoov.
6. Hloov nrog cov hmoov zoo - zoo.
6. Cua npuas thiab pinholes hauv txheej:
Ua rau:
1. Muaj qhov cua ntawm qhov chaw ntawm lub workpiece.
2. Cov kua ua kua seem muaj nyob rau saum npoo ntawm lub workpiece, degreasing los yog anti-kev kho xeb tsis tiav.
3. Lub conductive putty yog siv heev thickly thiab tsis tau qhuav tag.
4. Cov phom txau yog ze rau ntawm qhov chaw ua haujlwm, lossis lub zog ua haujlwm siab dhau lawm, ua rau cov txheej txheej tawg.
5. Cov pa hluav taws xob muaj nyob hauv qhov cub ci.
6. Txheej yog tuab heev los yog tsis kho tag nrho.
7. Teeb meem nrog cov hmoov txheej nws tus kheej.
Kev daws:
1. Txhim kho kev ua haujlwm thiab kho cov khoom ua haujlwm.
2. Txhim kho cov txheej txheem ua ntej.
3. ncua sij hawm ci.
4. Kho cov txheej txheem tsis.
5. Ntxuav lub qhov cub thiab ntxuav lub qhov cub kom huv.
6. Tswj txheej thickness mus rau 50-80 μm thiab kho kho tej yam kev mob.
7. Hloov nrog cov hmoov txheej tsim nyog.
7. Cov khoom siv tsis zoo ntawm cov txheej txheej, ua rau tag nrho cov txheej txheem tev tawm:
Ua rau:
1. Tsis zoo ntawm lub substrate los yog tsis tsim nyog pretreatment.
2. Kev ci tsis zoo, kho tsis tiav, lossis dhau - ci.
3. Cov hmoov tsis zoo, los yog cov hmoov tau dhau nws lub txee lub neej.
Kev daws:
1. Txhim kho pretreatment.
2. Txheeb xyuas cov txheej txheem ci tsim nyog.
3. Siv cov hmoov uas tsim nyog, thiab ua ib qho kev soj ntsuam tag nrho rau cov hmoov uas tas sij hawm.
8. Tsis zoo Corrosion Resistance ntawm txheej
Ua rau:
1. Cov txheej txheem tsis tau kho tag nrho.
2. Qhov kub tsis sib xws hauv qhov cub ci, qhov kub thiab txias sib txawv.
3. Kev kho tsis raug ntawm lub workpiece.
4. Kev ua haujlwm tsis zoo ntawm cov hmoov txheej.
Kev daws:
1. Kho qhov ci ci raws li kev ua haujlwm ntawm txheej txheej.
2. Xaiv lub qhov cub kom haum nrog qhov kub ntawm qhov sib txawv ntawm ± 5 ° C ntawm sab saum toj thiab hauv qab.
3. Ua kom muaj zog pretreatment thiab zam kev kho qhov seem ntawm qhov chaw ua haujlwm.
4. Hloov cov hmoov txheej uas tsim nyog.
9. Tsis zoo adhesion ntawm ya hmoov
Ua rau:
1. Lub tshuab hluav taws xob electrostatic tsis tsim hluav taws xob siab lossis qhov hluav taws xob tsis txaus.
2. Cov av tsis zoo ntawm lub workpiece.
3. Huab cua siab dhau.
4. Thaiv hauv cov kav dej ntawm cov khoom siv rov qab.
5. Ua tsis tiav pretreatment (xeb, roj).
6. Teeb meem nrog cov hmoov txheej nws tus kheej.
Kev daws:
1. Tshawb xyuas lub tshuab hluav taws xob electrostatic thiab kho qhov voltage.
2. Ntxuav cov khoom siv thiab tswj cov av kom zoo.
3. Kho cov cua siab.
4. Ntxuav lub cuab yeej rov qab.
5. Txhim kho cov txheej txheem ua ntej.
6. Siv cov hmoov txheej tsim nyog.
十. Cov hmoov tsis sib xws, txau cov nyiaj qee zaum siab, qee zaum qis
Ua rau:
1. Kev thaiv hauv zos hauv cov yeeb nkab hmoov, hmoov tsis zoo fluidity.
2. Cov cua tsis txaus, siab tsis ruaj khov.
3. Cov roj los yog dej sib xyaw hauv huab cua.
4. Tsis ruaj khov fluidization ntawm cov khoom siv hmoov, hmoov me me dhau ntawm cov khoom siv.
Kev daws:
1. Ntxuav cov khib nyiab los yog clumps hauv cov hmoov yeeb nkab, ua kom cov hmoov yeeb nkab tsis muaj kev cuam tshuam, thiab kho cov dej ntws ntawm cov hmoov txheej qhuav.
2. Xaiv lub tshuab cua compressor haum.
3. Tsis tu ncua tshem cov roj thiab dej ntawm lub tshuab cua compressor.
4. Khaws lub txaj fluidized cua siab ruaj khov thiab tsis tu ncua ntxiv cov hmoov tshiab.