Txhawm rau kom nrawm nrawm ntawm alkaline etching ntawm aluminium profiles, sodium nitrate lossis sodium nitrite, thiab cov khoom ntxiv xws li sodium gluconate, tuaj yeem muab ntxiv rau sodium hydroxide-raws li alkaline etching tov. Tsis tas li ntawd, yam xws li cov concentration ntawm cov tshuaj, qhov kub thiab txias, thiab lub sij hawm etching kuj muaj feem xyuam rau tus nqi ntawm industrial aluminium profile etching, nrog rau yuav ua li cas tswj cov yam ntxwv no.
Bath Solution Concentration:
Dissolving sodium hydroxide hauv dej tsim ib qho kev daws teeb meem alkaline, uas feem ntau yog siv hauv tshuaj ntxuav da dej rau txhuas profiles, tseem hu ua alkaline etching daws. Hauv alkaline etching daws, sodium hydroxide muaj nyob rau hauv lub xeev dawb ionic. Raws li qhov concentration ntawm sodium hydroxide nce mus rau 250 g / L, etching tus nqi ntawm industrial aluminium profiles kuj nce. Qhov no qhia tau hais tias qhov siab dua qhov concentration ntawm sodium hydroxide hauv da dej, qhov nrawm nrawm dua. Txawm li cas los xij, ntau lub tuam txhab tam sim no tswj cov ntsiab lus sodium hydroxide nyob rau hauv thaj tsam ntawm 50-100 g / L kom txuag tau nqi. Txhawm rau tswj cov ntsiab lus sodium hydroxide, gluconates tuaj yeem muab ntxiv rau lub neej ntev ntxiv, khaws cov ntsiab lus sodium hydroxide dawb hauv thaj tsam ntawm 70 g / L.
Aluminium Dissolution Tus Nqi:
Muab cov txhuas profile tso rau hauv cov tshuaj sodium hydroxide alkaline. Aluminium reacts chemically nrog sodium hydroxide los ua aluminium hydroxide. Lub xub ntiag ntawm cov khoom siv tshuaj tiv thaiv txo qhov corrosion ntawm aluminium. Cov kev sim tau pom tias thaum lub txhuas qhov sib tov yog 26 g / L thiab sodium hydroxide concentration yog 50 g / L, qhov kub thiab txias, qhov qeeb ntawm aluminium corrosion. Yog li ntawd, nyob rau hauv ib tug tas mus li da dej concentration, lub siab dua cov aluminium dissolution tus nqi, lub qeeb tus nqi corrosion, lub ntsiab lus ntawm aluminium dissolution tus nqi yog inversely proportional rau tus nqi corrosion. Tus nqi tsim nyog ntawm aluminium dissolution yuav tsum tau txiav txim siab los ntawm kev suav, ua tib zoo saib cov kev hloov pauv hauv chav da dej, thiab tswj cov nqi ntawm aluminium dissolution nyob rau hauv ntau yam raws li xav tau.
Da dej kub:
Los ntawm kev sim ntawm 6063 aluminium profiles, peb tau xaus lus tias qhov kub ntawm lub da dej nce, qhov alkaline corrosion ntawm txhuas kuj nce sai heev. Rau txhua txhua 10℃nce nyob rau hauv qhov kub thiab txias, cov tshuaj tiv thaiv corrosion ntawm txhuas doubles. Yog li ntawd, qhov kub thiab txias, qhov ceev ntawm alkaline corrosion ntawm aluminium profiles, lub ntsiab lus hais tias lub da dej kub yog ncaj qha proportional rau tus nqi corrosion. Qhov no yog vim qhov corrosion ntawm aluminium profiles hauv cov tshuaj alkaline yog cov tshuaj tiv thaiv exothermic, tso tawm txog 20 kW / m² ntawm tshav kub. Nws yog feem ntau tsim nyog rau nruab ib lub tshuab cua txias uas muaj peev xwm txaus los tuav lub da dej kub nyob rau hauv thaj tsam ntawm 50-60 degree; cov kab ke no tuaj yeem ua haujlwm ua khoom siv cua sov thaum lub caij ntuj no.
Lub sijhawm etching:
Nyob rau hauv cov tshuaj tiv thaiv alkaline etching, ntev lub sij hawm etching rau industrial aluminium profiles, ntau dua qhov hnyav ntawm aluminium dissolution. Txawm li cas los xij, lub sijhawm etching tsis ncaj qha ntsig txog qhov nrawm nrawm. Txo lub sij hawm etching tuaj yeem tsuas yog txo qhov hnyav ntawm aluminium dissolution thiab txo qhov noj ntawm alkaline etching agents, tab sis nws tsis yog proportional rau etching ceev. Txhawm rau ua kom tiav qhov chaw du ntawm aluminium profiles, cov neeg kho tshuab polishing lossis sandblasting tuaj yeem siv ua ntej, lossis ua tiav qhov ci thiab du tuaj yeem ua tiav los ntawm kev txhim kho qhov zoo ntawm pwm thiab txheej txheem extrusion.