Factors affecting the alkali erosion rate of aluminum profiles and control methods

Txhawm rau kom ceev cov alkali yaig ntawm aluminium profiles, sodium nitrate los yog sodium nitrite tuaj yeem muab ntxiv rau sodium hydroxide, thiab tom qab ntawd ntxiv cov khoom xws li sodium glutamate.

 

Da dej kom zoo

Cov sodium hydrocide yog yaj hauv dej los ua cov kua dej alkali nyob hauv lub taub dej alkali Cov concentration ntawm sodium hydroxide nyob rau hauv da dej, yog li cov ntsiab lus ntawm cov txiaj ntsig hydroxide yog nyob rau hauv ntau nyob rau hauv thaj tsam ntawm 70g / l.
 

Tus nqi ntawm txhuas yaj
Muab cov tshuaj txhuas profile hauv cov sodium hydroxide chinese, qhov kev sim ua pov thawj, qhov ua pov thawj ntawm cov khoom kub, nws tuaj yeem pom tau tias qhov ntau dua, qhov ntau dua, qhov ntau dua, qhov ntau dua ntawm cov khoom kub, nws tuaj yeem pom tau tias qhov kev pom zoo ntawm lub tank nyob Tsis hloov pauv, qhov siab dua tus nqi ntawm yaj aluminium, qeeb qeeb ntawm etching ceev, uas yog, tus nqi ntawm yaj aluminium yog qhov sib luag ntawm etching tus nqi. Nws yog ib qho tsim nyog kom tau txais tus nqi tsim nyog ntawm cov kev muab xam, ua tib zoo saib ntawm cov kua da dej txhuas hauv cov xwm txheej tshwj xeeb raws li qhov xwm txheej.

 

Tus da dej kub
Los ntawm kev sim ntawm 6063 cov ntaub ntawv txhuas, peb xaus lus tias nrog qhov kub thiab txias, yog li qhov ntsuas kub, kom ntau dua li ntawm lub tank, yog li qhov ntsuas kub thiab txias, yog li qhov kub thiab txias Qhov no yog vim qhov tseeb tias qhov kev sib xyaw ua ke hauv Alkali Kev daws teeb meem yog qhov ntsuas kub thiab txias, thiab nws feem ntau yog siv cov khoom siv cua txias

 

Lub sijhawm erodation
Hauv Alkali Etching Cov tshuaj tiv thaiv, ntev dua lub sij hawm ntawm alkali tsis muaj zog ntawm aluminium kev ua kom yuag, koj tuaj yeem ua thawj txoj kev ntawm cov tshuab Kev txhuam hniav lossis khau khiab los ua cov txheej txheem, lossis los ntawm kev txhim kho qhov zoo ntawm cov pwm thiab cov txheej txheem extrusion zoo kom ua tiav qhov ci thiab du nyhuv.