May 27, 2025 Tso lus

Yuav ua li cas koj lo aluminium rau pobzeb

How do you stick Aluminium to tile
How do you stick Aluminium to tile

Txhawm rau sib khi txhuas kom cov vuas, xaiv cov nplaum tsim nyog thiab ua raws cov ntaub ntawv 'cov khoom (cov khoom siv du, txhuas lub zog qis). Hauv qab no yog cov lus qhia tshaj lij:

1. Kev npaj saum npoo

Pobzeb Saum Toj

Ntxuav: Siv ib qho kev siv dej cawv (piv txwv li, isopropyl cawv lossis acetone) tshem cov hmoov av, roj, thiab grout seem. Rau glossy vuas, maj mam xuab zeb rau thaj tsam nrog120-220 grit SandpaperTxhawm rau tsim cov ntxhib los mos, txhim kho adhesion. So rov qab nrog daim ntaub huv kom tshem tawm cov khib nyiab.

Priming (Xaiv tau): Rau tsis - Cov vuas vuas vuas luaj (piv txwv li, epoxy lossis acrylic- los txhim kho cov nplaum ua kom zoo. Tso cai rau nws kom qhuav kiag li.

Aluminium Saum Toj

Ncab: Ntxuav nrog acetone los yog aluminium -}} Tshwj qhia rau tshem oxidation, roj, lossis cov chaw tsim khoom.

Nto etching: Txhawm rau txhawm rau txheej txheej txhuas oxide txheej thiab txhim kho adchesion:

Kev Siv Tshuaj Etching: Thov kev daws teeb meem ntawm5% phosphoric acidLos yog Aluminium etchant (piv txwv li, alodine) rau 1-2 feeb, tom qab ntawd yaug kom huv si nrog dej thiab qhuav.

NEEG KHO TSHUAB ETCHING: Xuab zeb lub txhuas nrog100-180 grit sandpaperlos tsim cov nplaim taws. Siv ntaub so ib daim ntaub so.}}}} Daim ntaub dawb tom qab.

 

2. Adhesive Xaiv

Xaiv cov nplaum raws li daim ntawv thov (sab hauv / sab nraud, thauj khoom {{{}} cov kabmob, ntsuas kub):

A. Epoxy adhesives

Rau haum: High {- lub zog ua rau hnyav {{{{} Lub luag haujlwm}, luas dim ntawm phab ntsa / plag tsev). Resistant rau dej, cua sov, thiab tshuaj lom neeg.

Hom:

Ob {- pе epoxy(Resin + Hardener): Sib tov hauv qhov sib npaug, thov nrog cov trowel lossis txhuam. Kho Sij Hawm: 24-48 teev (nyob ntawm seb qhov kub txias).

Epoxy - Raws li cov pobzeb nplaum(piv txwv li, mapi kerapoxy): tsim rau high-}} kev ua haujlwm sib haum; Qhov zoo tagnrho rau thaj chaw ntub dej (cov zaub mov ntub dej, chav ua noj).

Tus ntsis: Rau cov nplooj ntawv loj aluminium, sivEpoxy nrog muab tub lim(piv txwv li, silica) los sau cov khoob khoob.

B. Polyurethane Adhesive

Rau haum: Hloov pauv nyiaj rau thaj chaw nrog kev txav (xws li, cov vuas hauv pem teb nrog txhuas hloov). Resistant rau dej thiab UV hluav taws xob.

Tus yam ntxwv: Siaflex-252 (Marble / Hlau nplaum). Thov nrog rab phom caulking, clamp rau 12-24 teev.

Yam uas pab: Txuas hniav me me me me (txog li 3 hli) thiab tiv taus thermal expansion.

C. Acrylic -} raws cov nplaum

Rau haum: Lub teeb {{{{{0} plaub caug} Lub Luag Haujlwm Kev Siv (piv txwv li, Hniav Aluminium Panels rau phab ntsa). Yooj yim thov, ywg dej - tiv taus, thiab tsis - ua kom lom.

Tus yam ntxwv: Cov tes ua kua fuze nws tag nrho - cov nplaum. Thov nrog cov menyuam lossis txhuam, kho sijhawm: 24 teev.

Kev txwv: Qis dua kub tsis kam; tsis zoo tagnrho rau sab nraum zoov lossis sab nraum zoov.

D. Hloov Silicone Adhesives

Rau haum: Kev sib khi thiab tsev nyob hauv qhov chaw ntub dej (piv txwv li, txhuas da dej trims). Pwm - tiv taus thiab hloov tau.

Tus yam ntxwv: Ge silicone 2 chav ua noj & da dej. Thov siv hauv cov hlaws dai, cov cuab yeej nrog cov ntiv tes ntub, kho kom huv hauv 24 teev.

Tsab ntawv: SivNeutral -} Kho Siliconekom tsis txhob corrosion ntawm txhuas.

E. Cov Qauv Txheej Txheem (rau siab-} kev siv ntxhov siab)

Tus yam ntxwv: 3m scotch {{{}} weld dp8005 (acrylic {}} nyob) lossis loctite hysol ea ag 9394 (epoxy). Cov kev qhia no shear muaj zog txog 20 MPa thiab yog qhov zoo rau kev lag luam cov ntawv thov (piv txwv li, kos npe txhuas ntawm cov pobzeb facades).

 

3. Kev Ua Haujlwm Txheej Txheem

Thov Adhesive:

Rau me aluminium pieces (piv txwv li, siv adhesive ncaj qha rau cov txhuas siv cov tutel lossis cov koob txhaj tshuaj.

Rau cov nplooj ntawv loj, thov ib qho nyias nyias, txawm tias txheej txheem rau ob nplais thiab Aluminium cov chaw kom muaj kev sib cuag tag nrho.

Nias thiab Clamp:

Nias lub txhuas kom ruaj khov rau cov nplais, siv cov menyuam lossis roj hmab mallet kom tshem tawm cov pa npuas.

Rau cov khoom siv hnyav, siv clamps lossis tes taw hnyav los tso cai raws li kev ntsuas thaum lub sij hawm kho. Tshem cov pob zeb tom qab pib teeb tsa (xyuas cov lus qhia nplaum).

Kho sij hawm:

Tso cai rau cov nplaum kom kho tau siab (24-72 teev, nyob ntawm seb hom thiab ib puag ncig). Tsis txhob muaj dej los yog thauj khoom thaum lub sijhawm no.

 

4. Post {- becking checks

Kev Saib Xyuas Kev Pom: Txheeb xyuas qhov khoob lossis kev txiav txim siab. Coj mus rhaub cov txhuas kom mloog cov lus hollow, qhia tias tsis zoo adhesion.

Thauj Kuaj: Rau cov ntawv thov cov txheej txheem, thov cov roj av maj (piv txwv li, qhov hnyav) tom qab kho kom paub meej lub zog.

Sealing (yeem): Nyob rau sab nraum zoov lossis chaw ntub dej, thov kom cov Silicone Sealant nyob ib ncig ntawm cov npoo kom tiv thaiv cov dej ingress.

 

5. Kev Nyab Xeeb Kev Nyab Xeeb thiab ib puag ncig

Ua haujlwm nyob rau hauv ib tug zoo - pa thaj chaw; Hnav looj tes thiab kev tiv thaiv qhov muag thaum tuav tshuaj lom neeg.

Muab cov nplaum thiab cov tshuaj tua kom huv raws li cov cai hauv zos.

Rau cov ntawv thov sab nraum zoov, xyuas kom cov nplaum yog UV - tsis kam thiab nyob rau sab nrauv siv.

Cov qauv kev lag luam thiab kev coj ua zoo tshaj plaws

Ua raws li cov tuam txhab tsim cov txheej txheem rau cov khoom sib xyaw nplaum sib xyaw thiab kho lub sijhawm.

Rau kev lag luam cov haujlwm, cov ntawv yuam kev ntsuas lub zog ntawm cov qauv me me ua ntej kev teeb tsa tag nrho.

Nyob rau hauv kev tsim kho, xa mus rau cov qauv zoo li Ansi A108 (Pobzeb nyem) thiab ASTM D1002 (Shear Adhesion sim).

 

Los ntawm kev sib txuas ua ke npaj zoo, thiab txuas cov txheej txheem kho kom zoo, koj tuaj yeem ua tiav ib qho kev sib koom tes ruaj khov ntawm txhuas thiab cov vuas rau ob qho chaw nyob thiab cov ntawv thov kev lag luam.