Mar 19, 2025 Tso lus

Yuav ua li cas kom ua kom nce aluminium tsim thiab txuas lub neej ntawm extrusion tuag

e2b5045c061ca3ff84f185bbe40bfc0aba5ff4f747f2a-VBnKV0_fw658webp

Lub Neej Zoo Ntawm Txhuas Profile Pwm
Ua ntej kev ua tsis tiav ntawm cov pwm, tus naj npawb ntawm cov khoom tsim nyog tau tsim ua ntej ntawm pwm, thiab tus naj npawb ntawm cov khoom tsim nyog ua ntej kev kho cov pwm ntawm cov pwm uas tau hu ua thawj lub neej; Tus naj npawb ntawm cov khoom tsim nyog tau tsim tom qab ib qho kho ntawm cov pwm thiab ua ntej kho cov kev kho tom ntej yog hu ua lub neej kho. Pwm lub neej yog tus lej ntawm thawj lub neej thiab lub neej ntawm txhua txoj kev kho. Lub neej ntawm pwm yog cuam tshuam nrog cov duab thiab cov qauv ntawm cov pwm, thiab nws yog kev ua yeeb yam ntawm cov pwm, cov kev tsim khoom thiab cov pwm tsim khoom hauv ib lub sijhawm. Ib txoj kev xav txog ntawm qib ntawm kev kho cua sov ntawm cov pwm thiab qib kev siv thiab txij nkawm. Rau qee qhov tshwm sim, lub neej ntawm cov pwm ua kom pom cov qib ntawm kev lag luam metallurgical thiab kev lag luam machinery manrographical thiab machinery manufacturing kev lag luam hauv ib cheeb tsam thiab ib lub tebchaws.

Pwm tsis ua hauj lwm hom thiab cov tshuab

Txawm li cas los xij, muaj cov ntxhib peb hom tsis ua tiav, uas yog hnav, pob txha lov, thiab yas deformation.

(1) hnav thiab kua muag tsis ua haujlwm
Thaum cov pwm nyob hauv kev pabcuam, nws tau nkag rau hauv kev sib cuag nrog kev tsim cov khoob thiab tsim tawm suab lus tsa suab. Qhov tshwm sim ntawm kev paub txog kev sib tiv thaiv ntawm kev sib ze vim yog cov lus tsa suab txheeb ze ntawm cov npoo yog hu ua hnav. Puas ua txhaum kev ua tsis tiav tuaj yeem faib ua cov hom hauv qab no:

(2) Txhaum nyuaj tsis ua haujlwm
Thaum cov pwm muaj cov tawg loj lossis sib cais ua ob ntu thiab ntau qhov chaw thiab poob peev xwm ua haujlwm, nws dhau los ua pob txha lov. Kev ua kom tawg tau tuaj yeem muab faib ua cov pob yas thiab hloov me me. Cov khoom siv pwm yog feem ntau nruab nrab thiab lub zog loj hlau, thiab daim ntawv ntawm pob txha lov yog feem ntau brittle backstriav.
Nyeg pob txha tuaj yeem muab faib ntxiv ua ib qho {{}} lub sij hawm bacture thiab rog rog tawg.

(3) Yas deformation tsis ua haujlwm
Cov yas yas deformation ntawm cov pwm yog cov txiaj ntsig los ntawm cov khoom siv hlau ntawm cov pwm. Seb cov yas deform tshwm sim lossis tsis muaj yeej los ntawm cov neeg ua haujlwm thauj khoom thiab lub zog ntawm cov pwm ntawm chav sov. Seb cov pwm uas tau ua haujlwm ntawm qhov kub muaj cov tshuaj yej yas tsuas yog nyob ntawm kev ua haujlwm ntawm lub pwm thiab siab- lub zog ntawm cov pwm khoom. Nrog rau kev txhim kho cov kev lag luam txhuas kev ua lag luam, nyob rau hauv tsis ntev los no, txhua tus neeg tab tom nrhiav kev txhim kho qauv zoo dua thiab txuag tau zoo thiab nce cov txiaj ntsig thiab nce cov txiaj ntsig thiab nce cov txiaj ntsig thiab nce cov txiaj ntsig thiab nce cov txiaj ntsig thiab nce cov txiaj ntsig thiab nce cov txiaj ntsig thiab nce cov txiaj ntsig thiab nce cov txiaj ntsig thiab nce cov txiaj ntsig thiab nce cov txiaj ntsig thiab nce cov txiaj ntsig. Rau cov zis ntawm aluminium profiles, exustrusion tuag yog tsis ntseeg qhov tseem ceeb tswj node. Txhawm rau txhim kho nws lub neej yog ntawm cov teeb meem system system, feem ntau ntawm cov txheej txheem tsim tawm, feem ntau los ntawm kev tsim kho, siv thiab kev saib xyuas thiab lwm yam tseem ceeb tshaj plaws.