Tus neeg twg uas ua extruded aluminium profiles paub tias scrapping qhov profile thaum nws yog bent yog heev tsis tau paub, thiab nws yuav zam tau! Yog li, yuav ua li cas txo lossis zam kev txhuam vim khoov?
Extrusion ncaj:Ncaj kev yog qhov sib txuas heev tshwm sim los ntawm cov ntaub ntawv, cov neeg ua haujlwm kom ncaj yuav tsum ua kom muaj zog, thiab lwm yam.,
Extrusion thiab Framing:Qhov txuas txuas no tseem yog qhov tseem ceeb heev, tom qab pom qhov ntev ntawm tus pas ntsuas, nws yog qhov tsim nyog yuav tsum tau uates, thiab cov khoom lag luam tsis zoo lossis yog cov khoom siv nrog cov kav dej lossis cov khoom siv ua ke? Feem ntau hais lus, tus ncej ntawm ob qho kawg ntawm cov ntaub ntawv loj thiab cov khoom siv nrog cov khoom siv me me thiab cov khoom rub tawm ntawm cov khoom me me thiab lub tiaj pwm yog qhov yooj yim los khoov ntawm ob qho kawg. Txawm li cas los xij, qee qhov profiles tsis zoo txawm li ntawd, xws li cov lototer, cov khoom siv lub qhov rai, gland yuav tsum muab tso rau hauv cov profiles laus thiab tom qab ntawd nqa mus rau hauv ncej.
Nto kho ntawm lub txee:Lub billet yog hnub nyoog, lub hardness tau mus txog tus qauv, qhov profile tsis yooj yim los khoov rau qhov tseeb, sim kom tsis txhob mloog zoo li kev sib txawv, nws tseem yuav tsum tau them rau lub txee, nws tseem yuav tsum tau them rau lub txee, nws tseem yuav tsum tau them rau lub txee, nws tseem yuav tsum tau them rau lub txee, nws tseem yuav tsum them rau lub txee, nws tseem yuav tsum them rau lub txee, nws tseem yuav tsum them rau lub txee, nws tseem yuav tsum them rau lub txee, nws tseem yuav tsum tau them rau lub txee, nws tseem yuav tsum tau them rau lub txee, nws tseem yuav tsum tau them rau lub txee, nws tseem yuav tsum tau them rau lub txee, nws tseem yuav tsum them rau lub txee, nws tseem yuav tsum tau them rau lub txee, nws tseem yuav tsum tau them rau lub txee, nws tseem yuav tsum tau them rau lub txee, nws tseem yuav tsum them rau lub txee, nws tseem yuav tsum tau them rau lub txee, nws tseem yuav tsum tau them rau lub txee, nws tseem yuav tsum tau them rau lub txee, nws tseem yuav tsum tau them rau lub txee, nws tseem yuav tsum tau them rau lub txee, nws tseem yuav tsum tau them rau lub txee, nws tseem yuav tsum tau them rau lub txee, nws tseem yuav ua rau muaj kev hloov pauv zoo, nws tseem yuav ua rau muaj kev hloov pauv ntawm cov laus.