Increase extruded aluminum profile output through temperature control

 

Feem ntau thaum tsis muaj kev tshem tawm hauv lub sijhawm, cov zis tshaj plaws yog kev txiav txim siab nrawm nrawm, uas yog hloov pauv thiab lwm tus kuj hloov tau. Thawj qhov yog qhov kev sib zog sib zog ntawm cov extruden, uas tuaj yeem nyem tau yooj yim thaum lub zog ingot yog tsawg thaum lub zog extrusion loj; Qhov thib ob ntawm kev tsim qauv, kev sib txhuam ntawm cov hlau thiab cov pwm ntawm cov raj hluav taws xob thaum muaj qhov kub ntawm aluminium almoy los ntawm 35 ~ 62 degree; Qhov thib peb yog cov yam ntxwv ntawm extruded alloy, uas yog ib qho tsis muaj zog, thiab txawm tias txhuas feem ntau yuav tsum tsis pub dhau, lub zog, pwm, kua muag, thiab lwm yam. Qhov kawg ntawm qhov ntsuas kub thiab qhov ntsuas tau zoo npaum li cas nws tau tswj hwm.

 

Yog tias qhov kev sib zog sib zog ntawm cov profile profile tsis loj, nws yog qhov kub ntxhov, tab sis qhov kub ntawm lub qhov hluav taws xob tuaj yeem tiv thaiv qhov hluav taws xob kub ntawm cov khoom los ntawm kev ua siab dhau. Txhua tus alloy muaj nws tus kheej txoj kev ua kom sov rau qhov kub thiab txias. Kev xyaum ntau lawm tau ua pov thawj tias qhov ntsuas kub ntawm cov kev ncua cov npe yuav tsum khaws cia kom muaj li ntawm 430℃(thaum lub expusion ceev ntau dua los yog sib npaug rau 16 hli / s). Lub pwm kub ntawm 6063 alloy profiles yuav tsum tsis pub tshaj 500 degree, qhov zoo tshaj plaws yog 512 kev ntsuas kub ntawm 6061 alloy yuav tsum tsis txhob loj dua 525 degree. Qhov hloov me me hauv cov pwm ua ke yuav cuam tshuam rau cov zis thiab cov khoom lag luam zoo.

Qhov kub ntawm lub rooj tog extrusion extrusion kuj tseem ceeb heev, tshwj xeeb tshaj yog saib rau qhov kub ua kom tiav, thiab nws yog qhov zoo tshaj plaws los ua kom muaj qhov kub thiab txias rau lub sijhawm ua haujlwm nyob rau tib lub sijhawm. Tus nqi preheating yuav tsum tsis txhob muaj ntau dua 38℃/ h. Qhov zoo tshaj plaws preheating specification yog: nce mus rau 23H degree, kom sov kom sov txog 430 degree, kom sov rau 4H, thiab tom qab ntawd muab tso rau hauv kev ua haujlwm. Qhov no tsis tsuas yog ua kom muaj kev sib haum xeeb thiab xwm txheej sab hauv thiab sab nraud, tab sis kuj muab sijhawm txaus kom tshem tawm txhua yam kev ntxhov siab hauv sab hauv thermal. Ntawm chav kawm, cua sov Extrusion lub tog raj kheej hauv qhov cub yog qhov zoo tshaj plaws rau preheat.

 

Thaum lub sij hawm cov txheej txheem extrusion, extrusion lub ntiaj teb kub yuav tsum yog 15 ~ 40℃qis dua li ingot kub. Yog tias qhov nrawm nrawm nrawm nrawm heev yog li ntawd extrusion lub ntiaj teb kub, nws yog ib qho tsim nyog los txo cov haujlwm daws teeb meem, tab sis kuj txo cov zis. Thaum lub sij hawm nce nyob rau hauv kev ceev nrawm, cov cua sov kev tswj hwm los ntawm ob peb raug txiav, tab sis extrusion lub ntiaj teb kub tseem tab tom nce. Yog hais tias extrusion lub ntiaj teb kub yog siab tshaj 470 degree, lub Extrusion Seem yuav sawv. Lub zoo tagnrho Extrusion Lub Zog Lub ntiaj teb qhov yuav tsum tau txiav txim siab raws li cov khoom sib txawv.

Tsis txhob xav tias preheating extrusion lub tog raj kheej yog qhov pov tseg ntawm lub sijhawm thiab lub zog. Txhawm rau ntes tau nrog txoj haujlwm ntau lawm, lub Hoobkas cua nrog sab hauv kev tiv thaiv ntawm ib sab, thiab ntawm qhov tod tes, nws ua kom sov nrog roj liquefied. Hauv qhov xwm txheej no, qhov ntsuas kub tsis tuaj yeem ntsuas thiab tswj tau, thiab cov khoom nthuav dav dua, thiab lub tog raj kheej nrawm dua, ua rau lub tog raj kheej tsis sib xws thiab hnov ​​ib qho "suab".

Qhov kev sib txuas ntxiv yuav ua rau sab hauv kev ntxhov siab thaum lub sijhawm ua haujlwm, uas yuav ua rau qaug zog tawg rau qee zaum tsis yog {{} Axial radial quab yuam. Yog li ntawd, tom qab kev coj ua lub sijhawm ua haujlwm ntawm kev kho kom zoo rau 4500H, nws yog qhov sov rau 1230, thiab tom qab ntawd nws txias nrog rau hauv qab 50℃nrog lub cub tawg.

 

Thaum tsim cov khoom lag luam saum npoo av, qhov ntsuas kub ntawm kev rho tawm cov ntaub qhwv kom txo tau cov suab ntawm cov suab nrov. Qhov zoo tshaj ntawm cov tapital extrusion Pad yog ntau dua zoo dua li qhov kev txav, thiab nws tuaj yeem txo cov cua sov ntxiv thiab txo cov kev nkag mus rau hauv cov ntaub ntawv, uas pab kom nce cov txiaj ntsig.

Cov pwm kub ua yog lub luag haujlwm tseem ceeb hauv kev tau txais cov zis ntau, feem ntau tsis qis dua 430 degree; Ntawm qhov tod tes, nws yuav tsum tsis txhob siab dhau, txwv tsis pub, tsis tsuas yog lub hardness yuav txo qis, tab sis kuj oxidation, feem ntau yog nyob hauv thaj chaw ua haujlwm. Thaum lub sij hawm lub tshuab ua kom lub cev ua kom muaj cov txheej txheem pwm, tsis txhob sib cuag ze ntawm cov pwm los thaiv cov kev ncig cua. Nws yog qhov zoo tshaj plaws los siv lub thawv cua sov cua sov nrog ib daim phiaj, thiab txhua tus pwm tso rau hauv ib lub thawv.

 

Qhov kub ntawm lub ingot billet thaum lub sij hawm ingot thaum lub sij hawm extrusion cov txheej txheem tuaj yeem ncav cuag txog 40℃lossis siab dua, thiab nce ntxiv los ntawm cov pwm tsim. Txhawm rau kom tau txais cov zis tshaj plaws, txhua qhov kub yuav tsum tsis quav ntsej, thiab txhua qhov kub yuav tsum tau sau thiab tswj qhov kub thiab txias kom pom qhov kev sib raug zoo ntawm lub tshuab thiab txhua qhov kub.

Cov neeg ua haujlwm ntawm Aluminium Extrusion Cov nroj tsuag ntau lawm cov nroj tsuag ntau lawm yuav tsum nco ntsoov tias kev tswj qhov kub ntawm yog qhov tseem ceeb kom tso zis ntxiv.