Nce cov zis ntawm extruded txhuas profiles los ntawm kev tswj qhov kub.

Increase the output of extruded aluminum profiles through temperature control.

Feem ntau, yog tias tsis muaj kev tshem tawm downtime, cov zis ntau tshaj plaws yog txiav txim siab los ntawm plaub yam, peb uas yog tas li thaum ib qho kuj sib txawv. Thawj qhov ua yog qhov kev tshem tawm siab ntawm extruder; Siab extrusion siab tuaj yeem tso cai rau kev zam kom muaj kev tiv thaiv kom deb ntawm qis dua ntawm lub billet. Qhov thib ob ntawm qhov yog tus tsim qauv tsim; Thaum lub sij hawm extrusion, kev sib txhuam ntawm cov hlau thiab cov tuag phab ntsa tau feem ntau nce qhov kub ntawm aluminium alloy los ntawm 35 txog 62 degree. Qhov thib peb yog cov yam ntxwv ntawm extruded alloy, uas yog ib qho kev tswj tsis tau zoo uas txwv qhov kev txiav txim siab ceev; Qhov ntsuas kub tawm ntawm cov profile feem ntau tsis tau tshaj 540 degree, thiab teeb meem xws li txhuas los, micro {}} Cov kab nrib pleb, thiab kua muag yuav tshwm sim. Qhov kawg ntawm qhov yog qhov kub thiab nws qib kev tswj hwm.

Yog hais tias qhov extrusion siab ntawm txhuas profile extruder yog tsis muaj zog txaus, nws yuav nyuaj rau kev tawm tsam zoo lossis txawm tias ua rau tuag txhaws qhov twg cov khoom txav. Hauv cov xwm txheej zoo li no tuaj yeem nce ntxiv, tab sis cov extrusion ceev yuav tsum qis dua los tiv thaiv qhov kub ntawm cov khoom uas tau dhau. Txhua tus Alloy muaj nws txoj kev coj zoo tshaj plaws (ingot) kub. Kev coj ua ntau lawm tau pom tias ingot kub yog kev tswj kom zoo tshaj plaws nyob ib ncig ntawm 430℃(thaum lub expusion ceev loj dua los yog sib npaug rau 16 hli / s). Qhov ntsuas kub tawm ntawm 6063 alloy profiles yuav tsum tsis pub tshaj 500 degree, thaum qhov kub siab tshaj plaws rau 6005 alloy yog 512 alloy, nws yog qhov zoo tshaj plaws tsis tau tshaj 525 degree. Kev hloov pauv hauv qhov ntsuas kub tawm tuaj yeem cuam tshuam cov khoom muag tawm thiab ua tau zoo.

Qhov ntsuas kub ntawm extrusion barrel kuj tseem yog qhov tseem ceeb heev, tshwj xeeb tshaj yog thaum lub sijhawm preheating; Nws yog qhov tseem ceeb los them sai sai rau qhov nce hauv qhov kub kom tsis txhob muaj kev ntxhov siab ntau ntawm cov khaubncaws sab nraud povtseg. Nws yog qhov zoo tshaj plaws los tsa cov extrusion barren thiab tes tsho rau kev ua haujlwm kub ib txhij. Tus nqi preheating yuav tsum tsis pub tshaj 38℃/ h. Qhov zoo tshaj plaws preheating raws tutorocol yog los nce qhov kub txog 235 degree, tuav nws mus rau 830℃thiab tuav tau 4 teev ua ntej pib ua haujlwm. Qhov no tsis tsuas yog ua kom muaj kev phom sij sab hauv thiab sab nraud tab sis tseem muaj sijhawm txaus los tshem tawm txhua qhov kev ntxhov siab sab hauv. Ntawm chav kawm, cua sov extrusion bimren nyob rau hauv lub cub hluav taws yog txoj kev zoo tshaj plaws rau preheat.

Thaum lub sij hawm cov txheej txheem extrusion, qhov kub ntawm extrusion barrel yuav tsum 15 txog 40℃qis dua qhov ntsuas kub ntawm ingot. Yog tias qhov nrawm nrawm nrawm nrawm nrawm, ua rau qhov kub ntawm cov expusion barrel mus rau ingot ntsuas kub, ntsuas yuav tsum tau ua kom qis dua qhov kub ntawm extrusion barrel. Qhov no tsis yog ib txoj haujlwm daws teeb meem, tab sis nws tseem yuav txo qis kev tawm. Raws li cov khoom lag luam ceev nce ntxiv, qee zaum cov cua sov tau tswj tau los ntawm thermocouple yuav raug txiav tawm, tsis tau qhov kub ntawm extrusion barrel tseem sawv. Yog hais tias qhov ntsuas kub ntawm extrusion barel tshaj 470 degree, tus nqi ntawm extrusion pov tseg yuav nce ntxiv. Qhov zoo tshaj plaws kub ntawm extrusion barrel yuav tsum tau txiav txim siab raws cov alloys sib txawv.

Tsis txhob xav tias preheating extrusion lub tog raj kheej yog qhov pov tseg ntawm lub sijhawm lossis lub zog. Thaum rushing cov haujlwm ntau lawm, ntawm ib sab tes, sab hauv cov Cheebtsam yog siv rau cua sov, thaum ntawm qhov tod tes hlawv rau cov cua sov. Hauv qhov xwm txheej no, qhov ntsuas kub tsis tuaj yeem ntsuas thiab tswj tau qhov kub thiab txias dua li cov khoom siv hluav taws xob sab nraud, ua rau lub suab sib txawv, ua rau lub suab sib txawv, ua rau lub suab sib txawv, ua rau 'tawg paj.

Thaum lub sij hawm ua haujlwm ua haujlwm, cov ncej Extrusion yuav nthuav kev ntxhov siab sab hauv sab hauv. Thaum cov kev ntxhov siab no tau nce mus txog qee theem, nkees tawg yuav tshwm sim, thiab nws tuaj yeem tsoo hauv qab tsis yog}} Axial radial rog. Yog li ntawd, tom qab cov kev coj ua lub sijhawm ua haujlwm ntawm kev kho kom haum 4500, nws yog qhov ntsuas kub ntawm 430 txog 12 teev, tom qab ntawd txias rau hauv qab 50℃hauv qhov cub.

Thaum tsim cov khoom lag luam nto, ntsuas kub ntawm kev rho tawm cov khoom siv tsis xws luag nrog cov khoom lag luam uas tsis sib xws nrog cov suab nrov nto. Qhov zoo ntawm kev hloov pauv cov ntaub ntawv zoo dua li ntawm cov khoom siv tau txias, vim tias lawv tuaj yeem khaws cov cua sov ntxiv, uas txo qis ntawm cov impurities rau hauv qhov profile, pab txhim kho kom muaj txiaj ntsig.

Qhov ntsuas kub ntawm cov pwm ua lub luag haujlwm tseem ceeb hauv kev ua tiav cov khoom tsim tau zoo, feem ntau yuav tsum tsis txhob qis dua 430 degree; Ntawm qhov tod tes, nws yuav tsum tsis txhob siab dhau, txwv tsis pub, tsis yog tsuas yog cov tawv tawv txo qis, tab sis kuj oxidation yuav tshwm sim feem ntau hauv thaj chaw ua haujlwm. Thaum lub cev cov txheej txheem cua sov, pwm yuav tsum tau muab sib nrug kom tsis txhob muaj kev cuam tshuam ntawm huab cua ncig.

Qhov kub ntawm lub billet thaum lub sij hawm extusion tuaj yeem nce txog 40℃lossis ntau dua, thiab nce ntau yog nyob ntawm cov pwm tsim. Yuav kom ua tiav cov zis tshaj plaws, nws yog qhov tseem ceeb tsis txhob ua kom dhau ntau yam kub; Txhua qhov kub yuav tsum tau sau tseg thiab nruj me ntsis tswj hwm kom txiav txim siab qhov kev sib raug zoo ntawm lub tshuab siab tshaj plaws thiab ntau qhov kub.

Thaum kawg, cov neeg ua haujlwm ntawm Aluminium Profile Extrusion Cov Hoobkas ntau lawm yuav tsum nco ntsoov tswj qhov kub thiab kev tswj tau zoo rau kev nce qib.