Cov txheej txheem khiav lag luam rau txhuas extrusion presses

Aluminium extrusion presses:

1. Kuaj seb lub roj hluav taws xob zoo li cas thiab cov pa kub yog qhov qub.

2. Saib xyuas txoj siv txoj hlua, lub txaj txias, lub rooj rau kev puas tsuaj thiab khawb.

3. Ua ntej ncab, paub meej tias qhov ntev ntawm lub txhuas profile, thiab tom qab ntawd ces txiav txim siab qhov rub piv los txiav txim qhov ntev ntev. Lub txhuas khoom tsim hluav taws xob yog lub plhaub loj lub zog, feem ntau 6063T5 ncav yog 0.5% - 1%, 061 T6 rub Tus elongation yog 0.8% - 1.5%.

4. Paub qhov clamping method raws li cov duab ntawm txhuas profile. Qhov loj hollow profile yuav muab tso rau hauv lub tensile ncoo, tab sis sim ua kom ib qho chaw txaus clamping.

5. Thaum lub txhuas profile yog txias rau hauv qab 50 ° C, qhov profile yuav tsum stretched.

6. Thaum lub profile khoov thiab sib ntswg tib lub sijhawm, kev sib tw thiab khoov yuav tsum raug kho ua ntej.

7. Cov kev xeem thib ob thiab thib ob raug coj los xyuas kom paub tseeb tias qhov kev txiav txim siab thib ob thiab qhov clamping txoj kev tsim nyog. Pom kev khoov, twist, kos lub davhlau ya dav hlau, flare, thiab mus tib seem ntawm qhov profile. Yog tias nws tsis haum, kho lub ncab piv kom tsim nyog.

8. Yog tias lub cev tsis ncav tsis tseemceeb, tsis yog khawb, twisting, lossis thaum lub geometry tsis zoo, tus neeg tsav tsheb yuav tsum tau txais ntawv ceebtoom kom nres qhov kev rho tawm.

9. Cov profiles nyob rau hauv lub rooj txias txias yuav tsum tsis txhob txhuam, sib tsoo, sib tshooj thiab teeb, thiab tiv thaiv tau muab tshuaj ntxuav.

1.jpg



2_副本.jpg


Ua hauj lwm zoo ntawm cov extruder xovxwm aluminium thiab cov kev pab cuam lub neej muaj kev sib raug zoo nrog cov txheej txheem installation ntawm extruder. Ntxiv nrog rau qhov ua tau qhov hnyav ntawm qhov khoom siv thiab qhov nyhav ntawm cov ntaub ntawv raw cov khoom, cov khoom siv ntawm cov txheej txheem txhuas extrusion yog peev xwm ntawm lub siab qhov khoom ntawm nws tus kheej. Nws kuj yuav tsum tau txhawb nqa lub zog thaum lub extruder ua hauj lwm, yog li cov khoom siv yuav tsum tau muab nruab rau hauv raws li cov txheej txheem sib thooj.

Lus Cim

Tom qab siv lub tshuab hluav taws xob lawm, tus kws kho cov txheej txheem yuav tsum ua tib zoo nyeem cov khoom siv thiab, raws li cov kev cai hauv phau ntawv, tsim cov txheej txheem rau kev tsim khoom yas, siv cov txheej txheem khiav lag luam, kev npaj khoom, ntsuas cov cuab yeej thiab kev siv sijhawm. Nkag siab thiab paub txog cov qauv ntawm cov cuab yeej thiab kev ua haujlwm ntawm txhua feem, cim siv txhua khawm thiab hloov kev ua haujlwm.