Kev siv thiab tu ntawm Aluminium Extrusion tuag kom ntev lawv lub neej

Proper Use and Maintenance of Aluminum Extrusion Dies to Extend Their Lifespan

 

Lub neej ntev ntawm aluminium extrusion pwm tau dhau los ua qhov tseem ceeb hauv kev tsim kho ntawm Tuam Tshoj txoj kev lag luam aluminium profile. Kev tsim thiab tsim cov nqi ntawm aluminium extrusion pwm suav txog li 20% ntawm tag nrho cov nqi tsim khoom, ua rau nws yog ib qho ntawm cov thev naus laus zis tseem ceeb hauv kev lag luam aluminium extrusion, uas yog tus cwj pwm los ntawm kev hloov pauv thiab kev loj hlob sai. Nws koom nrog ntau yam xws li cov khoom siv, tsim, tsim, kev sim, kho pwm, thiab kev tswj hwm, thiab tseem yog ib qho ntawm cov cheeb tsam uas muaj peev xwm loj hlob.

 

Peb tuaj yeem siv hom kev hloov pauv pwm no zoo dua li cas? Peb tuaj yeem ua nws los ntawm cov hauv qab no.

 

(1) nruj me ntsis siv cov txheej txheem kev tsim khoom rau txhuas profiles

 

Nws yog ib qho tsim nyog yuav tsum nruj me ntsis ua raws li cov txheej txheem txhuas profile extrusion. Thaum pib, qhov kub ntawm qhov nruab nrab ntawm lub qhov cub hluav taws xob yuav tsum tau teem rau ntawm 530-550 degree, thiab qhov kub ntawm qhov hluav taws xob yuav tsum tau teem rau ntawm 480-500 degree. Lub sij hawm rwb thaiv tsev yuav tsum txaus los xyuas kom meej tias cov txhuas rods yog txaus rhuab thoob plaws (piv txwv li, ob qho tib si cov tub ntxhais thiab cov nto yog txaus rhuab). Qhov no tiv thaiv qhov kub tsis sib xws ntawm qhov chaw thiab cov tub ntxhais, uas tuaj yeem ua rau kom elastic deformation ntawm cov tuag, yog li ua rau qhov tshwm sim ntawm "cov phab ntsa tsis sib luag" thiab "ntev ntev," thiab tuaj yeem ua rau cov yas deformation ntawm extrusion tuag thiab nws cov seem.

 

(2) Xyuas kom 'Peb Lub Chaw Hauv Ib Leeg'


Lub hauv paus ntawm extrusion chim, tus pas nrig extrusion, thiab cov tuag yuav tsum visually concentric. Txhua qhov pom tseeb eccentricity tsis raug tso cai, vim tias nws tuaj yeem cuam tshuam tus nqi ntws hauv qhov sib txawv ntawm cov khoom, muaj peev xwm cuam tshuam cov khoom tsim, lossis ua rau ob sab ntawm cov khoom extruded sib txawv ntawm qhov ntev mus rau qhov chaw extrusion ntau lawm ua tsis tau.

 

Pwm puas tshuaj xyuas

① Cov khoom xaiv rau kev tsim cov pwm pwm tsis ua raws li cov kev xav tau ntawm kev ua haujlwm, ua rau pwm deform, corrode, lossis hnav hnyav tom qab ua haujlwm rau lub sijhawm.

② Thaum txhim kho lossis tshem tawm cov khoom ntawm cov pwm molding, hammering cov khoom tuaj yeem ua rau cov pwm pwm deform, ua rau cov khoom tiav, lossis tawm cov cim rau ntawm qhov chaw ua haujlwm.

③ Yog hais tias qhov ntws faib lub khob hliav qab lub kaum sab xis loj dhau, nws ua rau muaj kev tiv thaiv rau cov khoom siv molten, ua rau cov ribs ntawm cov dej faib lub khob hliav qab tawg.

④ Tsawg hardness ntawm qhov chaw ua hauj lwm ntawm cov tuag los yog mandrel tuaj yeem ua rau hnyav hnyav rau ntawm qhov chaw tiav, ua rau qhov chaw ntxhib.

⑤ Kev hloov pwm tsis raug tuaj yeem ua rau cov pwm hloov cov ntsia hlau tawg lossis deform lub tes tsho tuag los yog qhov loj me, ua rau lawv siv tsis tau.

 

(3) Kev xaiv zoo ntawm cov ntaub qhwv

 

Nws yog ib qho tseem ceeb uas yuav tsum xaiv qhov tsim nyog qhov loj me ob - qhov tshwj xeeb kev txhawb nqa pads kom txo tau qhov elastic deformation ntawm cov pwm qis, ua kom ruaj khov ntawm cov khoom extrusion nrog qhov sib txawv me me. Tsis tas li ntawd, ob lub - qhov tshwj xeeb cov ntaub qhwv yuav tsum tau npaj ua ntej cov pwm raug tshem tawm ntawm lub qhov cub kom tsis txhob muaj cua txias ntau dhau ntawm cov pwm vim lub sij hawm siv rau kev tshawb nrhiav cov ntaub qhwv, uas tuaj yeem ua rau pwm daig.

 

4) Txhim kho cov ntaub ntawv tawm tswv yim thaum lub sij hawm txhuas profile extrusion txheej txheem

 

A: Cov ntaub ntawv tawm tswv yim txog kev tuag ntsaws

 

Muaj ntau qhov laj thawj rau kev tuag ntsaws, thiab cov neeg tsis muaj kev cob qhia tshwj xeeb feem ntau pom tias nws nyuaj rau piav qhia meej. Nws yog qhov zoo tshaj plaws rau cov neeg ua haujlwm kho pwm cuam tshuam los ntawm tus kheej los tshuaj xyuas thiab txheeb xyuas qhov laj thawj ua ntej sim rov ua dua qhov tuag.

 

B: Cov lus teb rau Extrusion Moulding

 

Ntxiv nrog rau qhov muaj tus lej extrusion tuag kom meej meej cim rau ntawm lub billet, tag nrho cov kev taw qhia ntws ntawm lub billet, uas nyuaj rau kev pom, yuav tsum tau qhia rau nws. Piv txwv li: a. 'Converging extrusion' (qhia tias thaum lub sij hawm extrusion tiag tiag, sab hauv ntawm ob lub qhov txav qeeb dua sab nraud); b. 'Divering extrusion' (qhia tias thaum lub sij hawm extrusion tiag tiag, sab hauv ntawm ob lub qhov txav nrawm dua sab nraud); c. 'Sab laug ntev, txoj cai luv' qhia tias ceg laug ntev dua thiab ceg sab xis yog luv dua. Nws tseem yog ib qho tsim nyog los qhia qhov sib txawv ntawm qhov ntev vim tias qhov kev ncua deb ntawm qhov txiav tawm mus rau qhov hluav taws xob extrusion yog li 6 meters. Feem ntau, hom 'A meters / 6 meters' yog siv los qhia tias txhua txhua 6 meters, muaj qhov sib txawv ntawm A meters. Xws li cov ncauj lus kom ntxaws thiab meej yuav pab cov neeg ua haujlwm kho tuag ua kev txiav txim kom raug thiab ua haujlwm tu.

 

C: Cov lus teb rau ntau dhau qhov sib txawv:

Thaum ntsib ib qho xwm txheej uas cov extrusion molding yog ib txwm tab sis qhov ntev yog tawm, nws yog ib qho tseem ceeb uas yuav tsum tau coj ib tug qauv thiab kos nws nrog cov ntaub ntawv tiav thiab raug (extrusion pwm naj npawb, extrusion kev taw qhia, seem tsis xws luag, thiab lwm yam). Txhua qhov cim tsis raug tuaj yeem ua rau kho cov pwm tsis raug, yog li yuav tsum tau saib xyuas zoo.

Tsuas yog nrog cov lus qhia ua tiav ntawm kev siv tuaj yeem saib xyuas cov neeg ua haujlwm txiav txim siab thiab kho kom raug, txhim kho pwm kev ua haujlwm zoo, thiab txo tus naj npawb ntawm kev kho thiab tsis tsim nyog sim moldings.

 

 