(1) Cov txheej txheem cua sov ntawm aluminium alloy cam khwb cia pas nrig
Aluminium alloy cam khwb cia rods yog rhuab siv lub zog zaus induction cua sov. Cov yam ntxwv ntawm txoj kev cua sov no yog:
a. Lub sijhawm cua sov yog luv thiab tuaj yeem ncav cuag li 500℃hauv 3 feeb;
b. Lub extrusion kub yog tswj kom raug, thiab qhov yuam kev tsis tshaj ± 3 degree.
Yog tias lub qhov cub ua haujlwm tsis zoo siv los ua kom sov maj mam, theem Mg2Si yuav ua rau nag lossis daus, cuam tshuam cov nyhuv ntxiv.
(2) Aluminium profile extrusion
Cov hauv qab no tau hloov pauv mus rau kev tsim cov txheej txheem extrusion ntawm 6082 alloy aluminium profiles.
1. 6082 alloy muaj siab deformation tsis kam, yog li qhov kub ntawm cov pas nrig yuav tsum nyob rau sab saud (480-500 degree);
2. Qhov kub ntawm aluminium extrusion tuag yuav tsum siab;
3. Txhawm rau tiv thaiv kom tsis txhob shrinkage los yog kev koom tes ntawm npuas, oxide nplai, thiab impurities, lub siab residue yuav tsum tau tso tseg ntev dua;
4. Yuav kom yaj tag nrho lub ntsiab ntxiv dag zog rau theem Mg2Si nyob rau hauv lub alloy, lub quenching kub yuav tsum siab tshaj 500 degree. Yog li ntawd, extrusion tawm kub ntawm qhov profile yuav tsum tau tswj ntawm 500-530 degree;
5. 6082 aluminium alloy muaj siab quenching rhiab heev. Cov hlau muaj Mn, uas txhawb kev tsim cov intragranular intermetallic compounds thiab muaj kev cuam tshuam tsis zoo rau kev ua haujlwm quenching. Lub quenching txias siv yuav tsum muaj siab thiab qhov txias txias yog ceev, thiab qhov kub thiab txias yuav tsum tau txo kom qis dua 50℃los ntawm dej quenching;
6. Tom qab pom cov 6082 aluminium alloy profile, lub thav duab yuav tsum tau tiv thaiv ntawm ib qho kev ncua deb thiab yuav tsum tsis txhob tso tawm ntau dhau.