Qhov 'loj tawg' tsis xws luag hauv fluorocarbon coated aluminium cov ntaub ntawv thiab kev tiv thaiv kev ntsuas

The 'big cracking' defect in fluorocarbon coated aluminum materials and preventive measures

Cov xim fluorocarbon yog tsim los ntawm polytetrafluoroethylene resin, pigments, modifiers, thiab lwm yam. Hauv cov txheej txheem tsim khoom tiag tiag, cov txheej txheem yuav tsim kab -zoo li lossis kab sib chaws- zoo li cov kab nrib pleb zoo li lub pas dej qhuav; Qhov no tshwm sim yog hu ua 'loj cracking'. 'Kev tawg loj' feem ntau yog tshwm sim los ntawm cov kuab tshuaj tsis txaus thaum lub sij hawm yaj ntawm cov xim zaj duab xis thaum lub sij hawm ci tom qab txau. Cov xwm txheej hauv qab no yuav exacerbate qhov tshwm sim:

 

1. Lub sij hawm rau cov hlau saum npoo kub nce mus txog 235℃ntev dhau lawm;

 

2. Lub flash ziab ceev ntawm cov xim zaj duab xis ua ntej ci yog qhov ceev heev;

 

3. Cov profile yog tuab heev, thiab cov xim pleev xim yog tuab heev;

 

4. Cov ntsiab lus xim ntau dhau, xws li dawb lossis grey-dawb.

 

Cov kev ceev faj hauv qab no yuav tsum tau ua kom txo qis qhov tshwm sim ntawm "loj cracking":

 

1. Lub primer yuav tsum tsis txhob tsuag ntau heev thickly, nws yog pom zoo kom muaj ib tug qhuav zaj duab xis thickness ntawm 5-10μm;

 

2. Lub primer yuav tsum tsis txhob qhuav qhuav sai heev ua ntej yuav txau lub topcoat, txwv tsis pub, nws yuav ua rau hnyav absorbing ntawm lub topcoat. Ntxiv qeeb- cov kuab tshuaj kom qhuav tuaj yeem txuas ntxiv lub sijhawm ntub dej ntawm cov yeeb yaj kiab primer;

 

3. Lub topcoat yuav tsum tsis txhob tuab heev, nws yog pom zoo kom tsis txhob tshaj 35μm thiab evaporation yuav tsum tsis txhob ceev heev. Nws raug nquahu kom siv qeeb- cov kuab tshuaj kom qhuav, xws li glycol monobutyl ether lossis butyl carbitol; Feem ntau, nws lub sijhawm ziab ziab tsis tshaj 0.5 teev;

 

4. Cov txheej txheem ntawm cua sov rau lub cub tawg mus rau qhov kub thiab txias yuav tsum tsis txhob ncua; yog tias nws qeeb dhau los yog muaj qhov txias txias, nws tuaj yeem ua rau "loj tawg".