Txhuas phaj yog ntshiab txhuas phaj, uas yog 1 series, piv txwv li, 1060 belongs rau 1 series. Alloy Alloy Phaj tuaj yeem muab faib ua 7 Series, uas yog 2-8 Series. Piv txwv li, 2A21 belongs rau series 2, 3003 belongs rau series 3, 5052 belongs rau series 5, thiab lwm yam.
Qhov 1000 series yog cov ntshiab txhuas phaj, xws li 1060. Mus txog ntau dua 99%.
Qhov 2000 series yog daim ntawv txhuas nrog tooj liab ua lub ntsiab alloying. Cov ntsiab lus tooj liab tuaj yeem ncav cuag 2% -5%, lossis ntau dua, nyob ntawm daim ntawv thov. Lub hardness ntawm 2000 series yog tus txheeb ze rau lwm cov qib hauv Aerospace, lub 2000 series aluminium phaj tseem hu ua aviniation aluminium. Vim tias qhov tseeb tias cov neeg pej xeem yog tsis muaj peev xwm dav, muaj ntau yam me me tsim 2000 series Alloy Alloy Aluminium Ntawv. Ib yam li ntawd, tus nqi ntawm aluminium nplooj ntawv nyob rau hauv lub 2000 series yog qhov siab. Tam sim no, 5052 series tau hloov 2000 series nrog rau pej xeem sab.
Lub 3000 series yog cov phaj txhuas nrog manganese raws li lub ntsiab alloying. Cov ntsiab lus ntawm manganese yog nruab nrab ntawm 2 - 5%. Tus sawv cev ntau yam ntawm 3000 series suav nrog 3003 cov ntawv txhuas thiab 3A21 aluminium daim ntawv. Lub ntsiab yog vim li cas 3000 series aluminium phaj muaj qee cov tshuaj tiv thaiv xeb, thiab yog siv cov tshuab cua txias thiab tub yees. Tus nqi yog qhov zoo ua kom tau muab piv nrog lwm cov phaj alloy.
Lub 4000 series yog cov phaj txhuas nrog manganese raws li lub ntsiab alloying. Tam sim no, nws tsis yog siv dav.
Lub 5000 series yog ib tug sawv cev ntawm alloy aluminium daim hlau. Muaj ntau yog 5052, 5083 thiab lwm qib. Nws yog qhov feem ntau siv txhuas phaj nyob hauv Suav teb thiab lub ntiaj teb.
6000 series yog kev sib xyaw ntawm 4000 thiab 5000, cov ntsiab lus tseem ceeb suav nrog cov khoom seem uas muaj silicon thiab cov cim xeeb yog 6061-t6 aluminium phaj. Nws belongs rau cov khoom kub kub yaj kho cov txhuas phaj.
Qhov 7000 series yog 7075 raws li tus sawv cev tseem ceeb ntawm cov txhuas phaj. Feem ntau nyob rau hauv cov nqe lus ntawm hardness, kev ua tau zoo heev li ntawd ntawm 2000 series. Tsis nquag siv nyob rau lub sijhawm no.
Qhov 8000 series yog cov phaj txhuas nrog 8011 raws li tus neeg sawv cev tseem ceeb thiab lub ntsiab muaj nuj nqi ntawm lub raj mis cap, uas tsis nquag siv.