Jul 31, 2025 Tso lus

Qhov sib txawv ntawm cov paib txhuas thiab txhuas cov hlau txhuas

The distinction between aluminum plates and aluminum alloy plates

 

Txhuas phaj yog ntshiab txhuas phaj, uas yog 1 series, xws li 1060 belongs rau 1 series. Alloy Aluminium daim hlau tuaj yeem muab faib ua ke ua 7 koob, uas yog 2-8 Series. Piv txwv li, 2A21 belongs rau 2 series, 3003 belongs rau 3 series, 5052 belongs rau 5 series, thiab lwm yam.

 

Qhov 1000 series yog cov ntshiab txhuas phaj, xws li 1060. Lub ntsiab tivthaiv ntawm hom txhuas phaj yog txhuas. Cuag ntau tshaj 99%.

 

Qhov 2000 series yog daim phaj txhuas nrog tooj liab vim yog lub ntsiab lus sib xws. Cov ntsiab lus tooj liab tuaj yeem ncav cuag 2% -5% lossis siab dua nyob ntawm daim ntawv thov tshwj xeeb. Lub hardness ntawm 2000 series sib txheeb rau lwm qib hauv aerospace, txhuas tag nrho phaj ntawm 2000 series tseem hu ua aviniation aluminium. Vim tias tsis muaj kev pheej yig kev siv rau pej xeem, tam sim no muaj tsawg dua kev tsim 2000 series Alloy Alloy daim hlau. Ib yam li ntawd, tus nqi ntawm txhuas daim hlau nyob rau hauv lub 2000 series yog qhov siab. Tam sim no, 5052 series tau hloov 2000 series raws li kev siv pej xeem.

 

Lub 3000 series yog cov phaj txhuas nrog manganese raws li lub ntsiab alloying. Cov ntsiab lus ntawm manganese yog nruab nrab ntawm 2 - 5%. Tus sawv cev ntau yam ntawm 3000 series suav nrog 3003 ntawv nyeem thiab 3A21 phaj txhuas txhuas. Qhov loj tshaj plaws yog tias lub phaj txhuas ntawm 3000 series muaj qee qhov kev ua yeeb yam los tiv thaiv cov cua txias thiab cov tub yees. Tus nqi yog qhov zoo dua rau lwm cov phiaj hlau alloy.

 

Lub 4000 series yog cov phaj txhuas nrog manganese raws li lub ntsiab alloying. Nws tsis yog siv dav tam sim no.

Lub 5000 series yog ib tug sawv cev ntawm alloy aluminium daim hlau. Muaj feem ntau 5052 5083 thiab lwm qib. Nws yog feem ntau siv txhuas alloy phaj nyob rau hauv peb lub teb chaws thiab lub ntiaj teb.

6000 series yog kev sib xyaw ntawm 4000 thiab 5000, nrog cov ntsiab lus tseem ceeb nrog rau qib cua thiab cov neeg sawv cev tshiab yog 6061-t6 aluminium phaj. Nws belongs rau lub taag kub yaj kho cov txhuas phaj.

 

Qhov 7000 series yog 7075 yog tus sawv cev tseem ceeb ntawm cov txhuas phaj. Mas xav nyob rau hauv lub hardness, kev ua yeeb yam ze rau ntawm 2000 series. Tsis nquag siv thaum lub sijhawm.

Qhov 8000 series yog cov phaj txhuas nrog 8011 raws li tus neeg sawv cev tseem ceeb thiab lub ntsiab tseem ceeb ntawm kev ua lub raj mis caps, uas tsis nquag siv.