Tam sim no, tsis muaj qhov kev ntsuam xyuas ncaj qha los ua pov thawj kev sib raug zoo, tab sis cov txheej txheem extrusion thiab cov khoom ntawm cov yeeb yaj kiab oxide, thiab yog li qhov zoo ntawm kev sib khi.
Kev xyaum tau ua pov thawj tias qhov khoom zoo ntawm cov khoom tom qab oxidation thiab xim nyob ntawm ib sab ntawm cov khoom lag luam, nws yog qhov tsis muaj kev kho polishing.
The smooth and bright surface of the product is easy to obtain a satisfactory oxide film, uniform film thickness, good continuity, uniform distribution of film pores, and regular hole shape, such an oxide film not only has good physical properties, but also has high chemical activity, which has laid a good foundation for the smooth and reliable completion of the hole sealing.
Cov nplaim dej tsis zoo tsis yog cuam tshuam rau cov tsos, tab sis kuj feem ntau ua rau cov yeeb yaj kiab oxide, thiab lwm yam, thiab txawm tias tsis muaj cov khoom pov tseg uas tsis tuaj yeem ua haujlwm. Txhawm rau kom ntseeg tau tias qhov kev nce qib qis ntawm qis- kev ua yeeb yaj kiab thiab tsim cov qauv zoo ntawm GB / T5237-93 yuav tsum tau them rau cov hauv qab no hauv kev tsim khoom:
(1) Cov khoom lag luam zoo ntawm cov khoom seem yog lub hauv paus rau cov khoom siv kom zoo, thiab cov tshuaj oxidized, thiab cov teeb meem yuav tsum tau mus nqa tawm hauv lub sijhawm.
(2) Qhov ntsuas kub thiab tam sim no yuav tsum tau tswj tam sim no thaum muaj kev tsimxidation, tshwj xeeb tshaj yog qhov ntsuas kub yuav tsis siab dua 24 degree. Ntxuav tag nrho kom tsis txhob impurities raug coj tuaj rau lub torting tank.
(3) Yuav tsum muaj tus neeg tshwj xeeb tswj hwm lub tshuab xas, tswj cov neeg uas muaj nuj nqis, thiab saib xyuas cov tshuaj lom neeg fluoride, thiab saib xyuas qhov kev npaj thiab hloov kho ntawm lub tank kua.
(4) Sealing℃yuav tsum tau kuaj tom qab cov khoom tau muab tso rau 12 teev kom cov ntaub ntawv tuaj yeem yog qhov tseeb.