Cov txheej txheem plaub txheej txheem ntawm cov khib nyiab txhuas rov ua dua thiab ua tiav

The four basic processes of waste aluminum recycling and processing

 

Kev rov ua dua tshiab ntawm cov khib nyiab txhuas feem ntau suav nrog plaub txheej txheem hauv qab no.

 

(1) Kev npaj ntawm seem aluminium pib nrog thawj qhov kev faib tawm ntawm cov khoom seem aluminium, uas yog stacked los ntawm qib, xws li ntshiab aluminium, deformed aluminium alloys, casting aluminium alloys, thiab cov khoom sib xyaw. Rau cov khoom seem ntawm cov khoom siv txhuas, kev sib cais yuav tsum tau nqa tawm kom tshem tawm cov hlau thiab lwm yam tsis yog -ferrous hlau txuas nrog cov khoom siv txhuas, ua raws li cov txheej txheem xws li ntxuav, crushing, sib nqus sib nqus, thiab ziab kom tsim cov khoom seem. Rau lub teeb yuag, xoob, flaky qub txhuas qhov chaw, xws li lub xauv caj npab ntawm lub tsheb, lub tes tsho ceev, thiab aluminium shavings, lawv yuav tsum tau compacted rau hauv bales siv hydraulic hlau baler. Rau steel-core aluminium stranded hlau, cov tub ntxhais hlau yuav tsum tau muab cais ua ntej, thiab tom qab ntawd cov hlau txhuas yuav tsum raug mob rau hauv cov yob.

 

Hlau impurities muaj teeb meem heev rau smelting ntawm khib nyiab aluminium. Thaum cov ntsiab lus hlau yog siab dhau lawm, nws tuaj yeem tsim cov hlau tsis huv hauv cov txhuas, yog li txo nws cov khoom siv dag zog thiab ua rau nws tsis muaj zog corrosion. Cov ntsiab lus hlau feem ntau yuav tsum tau tswj kom qis dua 1.2%. Cov hmoov txhuas nrog cov ntsiab lus hlau ntau dua 1.5% tuaj yeem siv los ua cov deoxidizer hauv kev lag luam steel, thaum cov khoom lag luam muaj aluminium alloys tsis tshua siv khib nyiab aluminium nrog cov ntsiab lus hlau siab rau smelting. Tam sim no, tsis muaj txoj hauv kev ua tiav hauv kev lag luam txhuas uas tuaj yeem txaus siab tshem tawm cov hlau ntau dhau ntawm cov khib nyiab txhuas, tshwj xeeb tshaj yog hlau uas muaj nyob rau hauv daim ntawv ntawm stainless hlau.

 

Cov khib nyiab txhuas feem ntau muaj cov organic uas tsis yog{0}} hlau impurities xws li xim, roj, yas, thiab roj hmab. Ua ntej smelting hauv lub cub tawg, cov no yuav tsum tau muab tshem tawm. Rau hlau- hom khib nyiab txhuas, txoj hauv kev xws li kev sib tsoo tshuab, shearing tev, thermal tev, thiab tshuaj tev tawm feem ntau tuaj yeem ua haujlwm los tshem tawm cov rwb thaiv tsev. Tam sim no, cov tuam txhab lag luam hauv tsev feem ntau siv siab -kub ablation kom tshem tawm cov insulators, uas ua rau muaj roj ntau ntau thiab ua rau huab cua phem heev. Yog tias kev sib xyaw ua ke ntawm qis - qhov kub thiab txias yog siv, lub rwb thaiv tsev tuaj yeem softened nrog cov cua sov kom txo tau cov neeg kho tshuab lub zog, thiab tom qab ntawd mechanically rubbed tawm, ua tiav purification thaum tso cai rau cov ntaub ntawv rwb thaiv tsev rov qab. Cov coatings, roj stains, thiab lwm yam kab mob ntawm qhov chaw ntawm cov khoom siv khib nyiab tuaj yeem raug ntxuav nrog cov kuab tshuaj organic xws li acetone. Yog tias lawv tsis tuaj yeem raug tshem tawm, yuav tsum siv lub tshuab hluav taws xob pleev xim. Qhov kub siab tshaj plaws ntawm cov xim stripping rauv yuav tsum tsis pub tshaj 566 degree; tsuav yog cov khoom pov tseg nyob hauv qhov cub rau lub sijhawm txaus, cov roj thiab cov txheej txheem tuaj yeem raug tshem tawm tag nrho.

 

Rau cov ntawv txhuas ntawv ci, nws yog qhov nyuaj rau kev sib cais cov ntawv txhuas txheej los ntawm cov ntawv fiber ntau siv cov khoom siv khib nyiab zoo tib yam. Txoj kev sib cais zoo yog ua ntej tso cov ntawv txhuas ntawv hauv cov dej hauv cov dej, cua sov thiab nias nws, thiab tom qab ntawd maj mam ntws mus rau qhov qis - ib puag ncig kom txo qhov siab, ua raws li cov neeg kho tshuab nplawm. Txoj kev sib cais no tsis tsuas yog tso cai rau kev rov qab los ntawm fiber ntau pulp tab sis kuj tseem rov qab los ntawm aluminium ntawv ci.

 

Lub liquefaction thiab kev sib cais ntawm seem aluminium yog kev txhim kho yav tom ntej rau kev rov ua dua tshiab ntawm cov hlau txhuas. Nws muab cov khoom siv ua ntej ntawm cov khoom seem aluminium nrog remelting, uas tsis tsuas yog txo cov txheej txheem ntws tab sis kuj txo cov pa phem, thaum txhim kho qhov rov zoo ntawm cov hlau ntshiab.

 

Cov cuab yeej muaj lub lim uas tso cai rau cov pa roj kom dhau mus. Nyob rau hauv lub liquefaction txheej, txhuas precipitates nyob rau hauv qab, thiab cov organic tshuaj xws li cov xim uas txuas mus rau khib nyiab txhuas decompose rau hauv roj, tar, thiab cov pa roj carbon monoxide nyob rau hauv qhov kub siab tshaj 450 degree, uas yog ces tag nrho combusted nyob rau hauv lub oxidation ntaus ntawv nyob rau hauv lub separator. Cov khib nyiab yog nplawm los ntawm lub nruas rotating, tov nrog cov kuab tshuaj nyob rau hauv lub chamber, thiab impurities xws li xuab zeb thiab gravel yog sib cais rau hauv cov xuab zeb thiab gravel sib cais cheeb tsam, thaum lub yaj tov uas nqa tawm los ntawm cov pov tseg yog rov qab mus rau lub liquefaction chamber los ntawm lub rov qab ntsia hlau.

 

(2) Cov ntaub ntawv nyoos raug xaiv thiab suav raws li kev npaj thiab kev ua haujlwm zoo ntawm cov khoom seem aluminium, raws li cov kev xav tau ntawm cov khoom siv rov ua dua tshiab. Lub formulation yuav tsum coj mus rau hauv tus account lub℃ntawm oxidation thiab burning poob ntawm hlau, nrog silicon thiab magnesium muaj ntau oxidation thiab burning poob dua lwm yam alloying ntsiab. Qhov kub poob tus nqi ntawm ntau yam alloying ntsiab yuav tsum tau txiav txim siab sim ua ntej. Lub cev specifications thiab deg huv si ntawm seem aluminium yuav ncaj qha cuam tshuam rau qhov zoo ntawm cov khoom siv dua tshiab thiab cov hlau tawm los. Tsis zoo degreased seem txhuas tuaj yeem ua rau txog li 20% ntawm cov khoom siv tau zoo nkag mus rau hauv slag.

 

(3) Scrap aluminium alloys uas tuaj yeem ua rau deformed aluminium alloys suav nrog 3003, 3105, 3004, 3005, 5050, ntawm qhov tseem ceeb yog 3105 alloy. Txhawm rau kom ntseeg tau tias cov tshuaj lom neeg muaj pes tsawg leeg ntawm cov khoom siv hlau ua tau raws li cov kev xav tau thiab cov kev xav tau ntawm kev ua haujlwm siab, nws yuav tsum tau ntxiv qee qhov ntawm cov khoom siv txhuas txhuas.

 

(4) Tsuas yog ib feem me me ntawm cov khoom seem aluminium yog rov ua dua rau hauv deformed aluminium alloys; kwv yees li 1/4 yog recycled li deoxidizers rau steelmaking, thiab feem ntau yog siv nyob rau hauv recycled casting txhuas alloys. Tuag-casting aluminium alloys xws li A380 thiab ADC10, dav siv hauv Asmeskas thiab Nyij Pooj, yog qhov tseem ceeb siv los ntawm cov khoom siv txhuas.

 

Hauv cov txheej txheem rov ua dua tshiab ntawm cov khib nyiab aluminium, smelting thiab kho cov khoom siv rov ua dua tshiab yog cov txheej txheem tseem ceeb los xyuas kom meej qhov zoo ntawm cov khoom siv aluminium. Kev hloov kho thiab kho kom zoo ntawm txhuas yaj tuaj yeem tsis tsuas yog hloov cov morphology ntawm silicon nyob rau hauv aluminium-silicon alloys, purifying aluminium melting, tab sis kuj tseem txhim kho cov khoom ntawm aluminium alloys. Tam sim no, kev ua kom zoo thiab ua kom huv ntawm txhuas yaj feem ntau siv chlorides thiab fluorides xws li NaCl, NaF, KCl, thiab Na3AlF6, thiab qee qhov kev kho mob siv C12 lossis C2C16.