Qhov tseem ceeb ntawm kev laus kev kho cua sov hauv kev ua kom lub zog ntawm extruded aluminium

Kev kho cua sov ntawm aluminium yog txheej txheem tseem ceeb hauv aluminium profile factories thiab cov txheej txheem ntau lawm nrog cov kev cai nruj hauv kev cob qhia. Nws lub hom phiaj yog los hloov cov qauv sab hauv ntawm txhuas los ntawm cua sov, tuav, thiab txias, yog li ua tiav cov khoom xav tau. Cov cua kub sib txawv, tuav lub sij hawm, thiab cov txheej txheem txias yuav ua rau cov qauv sib txawv thiab cov khoom ntawm cov hlau, muab tso rau hauv cov kev kho cua sov sib txawv.

 

Deformed aluminium alloys tau muab faib ua ob pawg tseem ceeb: tsis yog- tshav kub- kho tau aluminium alloys thiab kub- kho tau aluminium alloys.

 

Kev Tiv Thaiv Kab Mob Tsis Zoo: Overheating: Qhov no yog hais txog kev puas tsuaj ntawm cov khoom siv kho tshuab los ntawm cov cua kub ntau dhau thiab tuav lub sij hawm ntev thaum kho cua sov, uas ua rau cov nplej ntxhib. Nws yog feem ntau kho siv cov txheej txheem normalizing. Overburning: Qhov no tshwm sim thaum cov cua kub kub siab dhau, ua rau tsis tsuas yog kev loj hlob ntawm cov qoob loo tab sis kuj tseem muaj cov ciam teb tsis muaj zog, xws li melting thiab oxidation ntawm grain ciam teb. Nyob rau hauv rooj plaub ntawm overburning, ntxiv rau cov qauv matrix pom zoo, cov oxides dub tau muab faib raws cov ciam teb. Cov khoom siv overburned tuaj yeem tsuas yog scrapped thiab remelted. Cov cua kub ntau dhau tsis tsuas yog ua rau cov nplej ntxhib xwb tab sis kuj ua rau cov oxidation hauv zos lossis melting ntawm cov ciam teb, ua rau cov qoob loo tsis muaj zog, hu ua overburning. Tom qab cov hlau yog overburned, nws cov kev ua tau zoo deteriorates hnyav, thiab tawg tuaj yeem tshwm sim thaum quenching. Cov qauv overburned tsis tuaj yeem rov qab tau thiab yuav tsum tau muab pov tseg. Yog li ntawd, nws yog ib qho tsim nyog kom tsis txhob overburning hauv kev ua haujlwm.

 

Dab tsi yog overheating? Dab tsi yog overburning? Dab tsi ua rau lawv? Lawv yuav tiv thaiv thiab kho li cas?
Teb:
① Overheating tshwm sim thaum cov cua kub kub siab dhau los yog cov khoom khaws cia ntawm qhov kub siab ntev ntev, ua rau cov nplej ntxhib. Tom qab quenching, tus qauv ua koob -zoo li.

② Kev kub nyhiab tshwm sim thaum lub cua sov kub siab dhau los yog cov khoom khaws cia ntawm qhov kub siab ntev ntev, ua rau oxidation nto ntawm lub workpiece. Overburned workpieces tsis tuaj yeem rov-quenched thiab yuav tsum tau muab pov tseg.

 

Yuav tiv thaiv li cas: Tshawb xyuas seb cov ntaub ntawv puas yog, tsim cov txheej txheem tsim nyog, ntsuas cov cuab yeej tswj hwm ua ntej kev kho cua sov, xaiv qhov kub kom zoo, tsis txhob nce qhov kub thiab txias los yog ncua sij hawm tuav ntawm koj tus kheej, tshaj tawm cov teeb meem hauv lub sijhawm. Kev kho: me ntsis overheated workpieces tuaj yeem kho tau los ntawm kev ncua lub sijhawm tempering. Hnyav overheated workpieces tuaj yeem ua rau normalizing cov nplej; Yog tias ib qho normalizing tsis kho cov nplej, qhov thib ob normalizing tuaj yeem ua tau, ua raws li kev kho cua sov raws li cov txheej txheem tsis tu ncua. Overburned workpieces tsis tuaj yeem kho thiab yuav tsum tau muab pov tseg.

 

Kev kho cua sov cov lis dej num: T1--Cov laus laus, T2--Annealing, T4--Tshuaj kho ntxiv rau ntuj laus, T5--Kev kho mob ntxiv rau kev laus tsis tiav, T6--Kev kho ntxiv ntxiv rau kev laus ua tiav, T7--Kev kho mob ntxiv rau kev kho kom ruaj khov.
Kev kho kev daws teeb meem: Hais txog cua sov cov hlau mus rau qhov siab - qhov kub ib zaug - theem cheeb tsam, tuav nws ntawm qhov ntsuas kub kom tso cai rau ntau theem kom yaj tag nrho rau hauv cov tshuaj tov, thiab tom qab ntawd maj mam txias kom tau txais cov tshuaj supersaturated.

Kev laus tsis tiav: Siv qhov kub tsis tshua muaj kev laus lossis lub sijhawm tuav lub sijhawm kom ua tiav tag nrho cov khoom siv dag zog zoo, lub ntsiab lus tseem ceeb ntawm lub zog, zoo plasticity, thiab toughness, tab sis corrosion kuj kuj yuav tsawg.
Ua kom tiav kev laus laus: Siv qhov kub thiab txias txias thiab tuav lub sijhawm ntev kom ua tiav qhov siab tshaj plaws hardness thiab siab tensile lub zog, tab sis nrog qis elongation.

 

Kev kho kom ruaj khov: Kev kho cua sov tsim los xyuas kom meej tias cov duab thiab qhov loj me ntawm cov khoom hloov pauv nyob rau hauv qhov txwv tsis pub dhau lub sijhawm ua haujlwm ntev -. Kev kho cua sov ntawm aluminium alloys txawv ntawm cov pa roj carbon steel; aluminium alloys muaj qhov tsis tshua muaj melting point, feem ntau ua rau overheating thiab hlawv, muaj qhov sib txawv me me ntawm cov cua sov, thiab xav tau qhov tseeb ntawm cov ntsuas kub ntsuas. Yog tias qhov cua sov thiab tuav qhov kub thiab txias deviates ntau dhau, lub hom phiaj ntawm kev ntxiv dag zog yuav tsis ua tiav.

 

Cov ntsiab lus hauv qab no yuav tsum tau sau tseg thaum lub sijhawm ua haujlwm:
1. Cov workpieces raug rhuab yuav tsum tau teem kom zoo nyob rau hauv lub cub tawg chamber, thiab lub cub tawg kub yuav tsum xyuas kom meej tias lawv yog rhuab tusyees.
2. Kev hloov kho kub muaj feem xyuam rau cov duab thiab qhov loj ntawm lub workpiece; Lub sij hawm hloov mus rau quenching yuav tsum luv li sai tau, feem ntau t < 6 vib nas this.
3. Nws yog qhov yuav tsum tau ua kom lub ntsuas kub ntawm lub qhov cub kho cua sov yog qhov zoo thiab ruaj khov hauv kev ua haujlwm, thaum tseem tsis txhob muaj qhov sib txawv ntawm qhov kub thiab txias los ntawm thermal inertia ntawm cov cua sov seem hauv lub cub tawg chamber. Qhov no xav kom peb saib xyuas thiab kho cov cua sov kom raws sijhawm. Los ntawm kev ua li ntawd, kev txhim kho kev ua tau zoo ntawm cov khoom ua haujlwm tuaj yeem ua tiav.

 

Deformable aluminium alloys uas tsis tuaj yeem ua kom muaj zog los ntawm kev kho cua sov yog cov uas nws cov ntsiab lus alloy ntog nyob rau hauv thaj tsam 1, los yog ob peb alloys uas nws cov ntsiab lus me ntsis dhau ntawm Zone 1 ntau, tab sis qhov kev txhawb zog tsis tseem ceeb. Cov alloys feem ntau muaj qhov zoo corrosion kuj thiab feem ntau hu ua xeb-resistant aluminium alloys. Lub ntsiab cua sov- kho tsis yog- muaj zog deformable aluminium alloys suav nrog ntshiab txhuas, Al-Mg series alloys, thiab Al-Mn series alloys. Piv txwv xws li 1060, 1050, 1100 (ntshiab txhuas), 5A02, 5A03, 5A06, 5056, 5456, 5083 (Al-}Mg series), thiab 3A21 (Al{25}}Mn series).

 

 