Aluminium Baseboard Strength Performance System Thiab Scene-raws li cov lus qhia xaiv

Ib. Core Strength Indicators thiab Substrate Benchmarks

Lub zog ntawm aluminium baseboards tau muab faib ua ob qhov loj:substrate inherent zogthiabcov khoom tiav tiav lub zog. Cov qub yog txiav txim siab los ntawm qib alloy thiab cov txheej txheem kho cua sov, thaum lub sijhawm tom kawg suav nrog kev sib xyaw ua ke ntawm cov qauv tsim, phab ntsa thickness, thiab kev kho saum npoo.

 

1. Mechanical Performance Standards for Substrates

Tshaj li 90% ntawm aluminium baseboards hauv kev lag luam yog extruded los ntawm 6063 series aluminium alloys. Cov khoom siv kho tshuab sib txawv heev nyob rau hauv cov kev kho cua sov sib txawv, thiab cov ntsiab lus tseem ceeb yuav tsum ua kom tau raws li qhov xav tau ntawm GB / T 5237.1-2017Aluminium Alloy Architectural Profiles - Part1: Substrates:

Cov khoom siv Tensile zog (MPa) Cov pov thawj muaj zog (tsis yog qhov sib npaug) (MPa) Elongation tom qab Fracture Brinell Hardness ntawm Substrate (HBW) Daim Ntawv Thov Scope
6063-T5 (Kev Lag Luam Txuj) Ntau dua lossis sib npaug li 175 Ntau dua lossis sib npaug li 130 Ntau dua lossis sib npaug li 8% Ntau dua lossis sib npaug li 60 Txuj rau kev siv vaj tse thiab kev lag luam dav dav
6063-T6 (High-Strength Qib) Ntau dua lossis sib npaug li 215 Ntau dua lossis sib npaug li 170 Ntau dua lossis sib npaug li 8% Ntau dua lossis sib npaug li 75 Cov tsheb loj thiab hnyav-load scenarios

Faj seeb: T5 hais txog cov txheej txheem ntawm cua txias + khoom aging tom qab extrusion forming, uas sib npaug lub zog thiab nto tsim zoo thiab yog cov txheej txheem thoob ntiaj teb rau cov hniav txhuas profile. T6 txais kev daws teeb meem quenching + kev laus laus, uas ua rau muaj zog ntau dua li ntawm 25% tab sis tuaj nrog ntau dua kev tsim nyuaj thiab nqi.

 

2. Kev ua tau zoo yuav tsum tau ua rau cov khoom tiav

Lub zog ntawm tiav aluminium baseboards yuav tsum ua tau raws li ob qho tib si cov txheej txheem mechanics thiab qhov kev puas tsuaj ntawm qhov yuav tsum tau ua. Raws li cov lus qhia tshwj xeeb rau kev kho kom zoo nkauj architectural aluminium profiles, cov khoom tsim nyog yuav tsum ncav cuag cov qauv hauv qab no:

Kev cuam tshuam tsis kam: Ntau dua los yog sib npaug ntawm 8J, muaj peev xwm tiv taus cov rooj tog zaum niaj hnub txav, ntxuav cov cuab yeej cuam tshuam, thiab kev sib tsoo ntawm cov neeg taug kev tsis muaj kev sib tsoo;

Flexural zog: Ntau dua los yog sib npaug rau 200MPa, tswj tsis muaj warping lossis deformation nyob rau hauv kev ntxhov siab ntev tom qab kev teeb tsa, nrog cov phab ntsa ruaj khov;

Nto cuam tshuam tsis kam: Ntau dua lossis sib npaug li 50kg·cm rau cov txheej txheem hmoov txheej, tsis muaj tev lossis tawg ntawm txheej tom qab cuam tshuam;

Nto hardness: Ntau dua lossis sib npaug rau HB50 rau lub substrate; txheej anodized zaj duab xis tuaj yeem ncav cuag 120 ~ 180HV Vickers hardness, tiv taus txhua hnub khawb thiab puas.

 

2. Plaub yam tseem ceeb cuam tshuam rau cov khoom tiav tiav

Nrog tib lub substrate, lub zog tiag tiag ntawm cov khoom tiav tuaj yeem sib txawv los ntawm ntau dua 40%, nyob ntawm qhov feem ntau ntawm peb cov qauv tsim: phab ntsa thickness, qauv, thiab txheej txheem.

 

1. Profile Phab ntsa Thickness: Qhov feem ntau intuitive zog sib txawv

Cov pa phab ntsa tuab hauv kev lag luam yog li ntawm 0.6mm txog 1.5mm, thiab phab ntsa tuab yog qhov zoo sib xws nrog cov hniav tsis kam thiab khoov tsis kam:

Cov khoom siv nrog phab ntsa tuab hauv qab 0.6 hli yog cov khoom siv tsis zoo-txo cov khoom, uas tuaj yeem deform nyob rau hauv tes siab thiab nws yooj yim rau loosening thiab qhov sib txawv widening tom qab installation;

Rau txhua txhua 0.2 hli nce nyob rau hauv phab ntsa thickness, kev cuam tshuam kuj txhim kho los ntawm kwv yees li 20% ~ 25%, ua nws txoj kev ncaj tshaj plaws los txhim kho lub zog.

"Nominal phab ntsa thickness exaggeration" yog dav nyob rau hauv kev ua lag luam. Piv txwv li, ib yam khoom uas sau 1.0mm yuav tsuas ntsuas 0.7 ~ 0.8mm. Thaum xaiv cov khoom, qhov tseeb phab ntsa thickness ntsuas los ntawm calipers yuav tsum yeej, es tsis yog tus tub luam tus nqi nominal.

 

2. Hla-Section Structure: Kev Pabcuam Tsis Pom Zoo

Lub ntsiab L-shaped cross-section nrog rov qab ob lub buckle grooves + transverse reinforcing ribs tuaj yeem cuam tshuam kev ntxhov siab, txhim kho khoov thiab warping tsis kam los ntawm ntau dua 25% piv rau cov ntaub ntawv tiaj tus yam tsis muaj tav. Qee cov khoom lag luam uas tsis tshua muaj peev xwm tshem tawm cov ribs sab hauv thiab tso siab rau ntawm daim hlau nyias nyias, uas ua rau cov wavy deformation tom qab siv mus ntev.

 

3. Txheej Txheem Kev Kho Hniav: Thib Ob Lub Zog Txhim Kho

Kev kho deg xws li anodizing thiab hmoov txheej tsis tsuas yog txhim kho kev zoo nkauj, tab sis kuj tsim cov txheej tiv thaiv tawv tawv ntawm txhuas nto:

Thaum cov anodized zaj duab xis thickness nce mus txog 10 ~ 25μm, deg hardness nce ho, thiab hnav thiab khawb kuj yog txhim khu kev qha;

Thick-film hmoov txheej tuaj yeem tsis cuam tshuam me me, txo qhov kev pheej hmoo ntawm substrate denting, thiab txhim kho corrosion kuj tib lub sijhawm.

 

4. Cov qauv kev teeb tsa: Qhov kawg lav ntawm lub zog

Buckled installation nrog expansion ntsia hlau fixation muab ntau yam kev ntxhov siab tis tshaj li cov nplaum installation, tsis txhob deformation los ntawm ib qho kev nyuaj siab. Lub nraub qaum roj hmab sawb zawj tuaj yeem tsis tsuas yog foob tiv thaiv cov dej noo tab sis kuj pab cuam tshuam cov phab ntsa cuam tshuam.

 

3. Phau ntawv qhia txog kev xaiv lub zog raws li Scenario

Raws li cov ko taw tsheb ceev thiab kev sib tsoo poob theem ntawm daim ntawv thov scenario, aluminium baseboards nrog sib txawv zog configurations yuav tsum matched raws li:

 

1. Cov xwm txheej nyob hauv

Cov chaw pa (chaw nyob, chav pw, kawm): 6063-T5 substrate nrog ntsuas phab ntsa thickness ntawm 0.8mm thiab txhawb nqa tav qauv raug pom zoo. Nrog rau kev khiav qis qis txhua hnub thiab kev sib tsoo feem ntau los ntawm kev tu cov cuab yeej thiab lub teeb rooj tog txav, qhov kev teeb tsa no ua tau raws li cov kev xav tau ntawm thaj chaw durability thiab yog qhov kev xaiv zoo tshaj plaws rau kev kho kom zoo nkauj hauv tsev.

Cov khoom siv hauv tsev siab (kev nkag, hauv tsev, tsev neeg nrog menyuam yaus / tsiaj): 6063-T5 substrate nrog ntsuas phab ntsa thickness ntawm 1.0mm yog pom zoo. Nws cov hniav thiab khawb tsis kam yog li 30% siab dua li 0.8mm version, muaj peev xwm tiv taus cov khoom ua si cuam tshuam thiab khawb tsiaj, ua kom zoo dua qub rau kev siv mus ntev.

 

2. Cov xwm txheej pej xeem ua lag luam

Kev siv dav dav (chaw ua haujlwm, khw me me, chav tsev so): 6063-T5 substrate nrog ntsuas phab ntsa thickness ntawm 1.0mm yog pom zoo. Nrog cov neeg ua haujlwm nruab nrab ntws thiab ntau zaus ntawm cov rooj tog zaum hauv chaw ua haujlwm thiab lub nra txav dua li cov chaw nyob, qhov kev teeb tsa no tuaj yeem tiv taus kev sib txhuam txhua hnub thiab kev cuam tshuam me me.

Cov chaw tsheb loj (cov khw muag khoom, khw muag khoom, tsev kho mob, tsev kawm txoj kev hauv tsev)6063-T5 substrate nrog ntsuas phab ntsa thickness ntawm 1.2 ~ 1.5 hli yog pom zoo; rau cov kev xav tau siab dua, nws tuaj yeem hloov kho mus rau 6063-T6 substrate. Nrog ntu ntu ntu thiab cuam tshuam los ntawm cov khoom siv hauv pem teb, trolleys, thiab lub nra, kev sib xyaw ua ke ntawm cov phab ntsa tuab + txhawb nqa cov tav tuaj yeem txo qhov kev saib xyuas thiab hloov zaus.

 

3. Muaj / Tshwj Xeeb Heavy-Load Scenarios

(Lub Hoobkas Rhiav, warehouses, underground garages, logistics passages) 6063-T6 high-strength aluminium alloy nrog ntsuas phab ntsa thickness ntawm 1.5mm thiab saum toj no yog pom zoo. Nrog rau kev pheej hmoo ntawm forklift thiab hydraulic tsheb hla dhau thiab cov khoom hnyav sib tsoo, lub siab-yield-strength substrate ua ke nrog cov qauv tuab-phab ntsa tuaj yeem tiv taus qhov cuam tshuam thiab dov los ntawm cov khoom hnyav, ua tau raws li kev lag luam-qib durability.

 

4. Kev lag luam xwm txheej thiab cov lus qhia txog kev txheeb xyuas zoo

Tam sim no, qhov pib nkag rau kev lag luam aluminium baseboard yog qhov tsawg. Qee cov tub lag luam txiav cov nqi los ntawm kev txo cov phab ntsa tuab, txo qis qib substrate, thiab ua kom yooj yim cov txheej txheem kho cua sov, ua rau cov khoom tsis zoo. Thaum kev yuav khoom thiab xaiv, qhov zoo tuaj yeem txheeb xyuas los ntawm peb lub ntsiab lus tseem ceeb:

Tshawb xyuas cov ntawv xeem: Yuav tsum muaj cov neeg muab khoom siv los muab cov ntaub ntawv ntsuas kev ua tau zoo nrog CMA daim ntawv pov thawj kom paub meej tias cov ntsuas tseem ceeb xws li lub zog tensile, lub zog tawm los, thiab kev cuam tshuam tsis zoo raws li cov qauv;

Ntsuas phab ntsa thickness thiab qauv: Ntsuas qhov tseeb phab ntsa tuab ntawm qhov profile nrog calipers, thiab xyuas seb puas muaj cov hlua txuas ntxiv thiab cov buckle grooves nyob tom qab;

Paub meej tias substrate identification: Qhia meej tias qib substrate yog 6063-T5 kom tsis txhob hla cov khoom siv rov ua dua tshiab lossis lwm yam txhuas ua cov khoom tsim nyog.

Raws li kev lag luam cov khoom siv kho kom zoo nkauj txhim kho mus rau qhov zoo, aluminium baseboards tau hloov zuj zus mus rau hauv cov kev taw qhia ntawm "siab zog nrog lub teeb yuag, customized qauv, thiab cov qauv kev ua tau zoo". Kev nthuav qhia lub zog qhia qhov system thiab cov qauv kev xaiv raws li qhov xwm txheej tsis yog tsuas yog lub hauv paus ntawm kev ua kom zoo ntawm qhov project, tab sis kuj yog tus yuam sij rau kev txhawb nqa lub suab ntawm kev lag luam.