Lub ntsiab alloying ntsiab ntawm 063 aluminium alloy yog magnesium thiab silicon. Nws muaj kev ua haujlwm zoo heev, zoo heev weldability, extrudability, thiab plating zog, zoo corrosion kuj, toughness, yog ib qho yooj yim rau polish, siv cov txheej saum toj kawg nkaus, thiab muaj cov teebmeem zoo anodizing. Nws yog ib tug raug extrusion alloy, dav siv rau lub tsev profiles, irrigation kav, tsheb khoom, rooj zaum, rooj tog, nqa, laj kab, thiab lwm yam kav dej, pas nrig, thiab profiles . 6063 feem ntau yog siv rau lub tsev profiles.

 

Lub ntsiab alloying ntsiab ntawm 6061 aluminium alloy yog magnesium thiab silicon, tsim Mg2Si theem. Yog tias muaj qee yam ntawm manganese thiab chromium, lawv tuaj yeem tiv thaiv qhov tsis zoo ntawm cov hlau; Qee zaum qee qhov me me ntawm tooj liab lossis zinc kuj tseem ntxiv los ua kom lub zog ntawm cov hlau tsis muaj qhov txo qis nws cov corrosion kuj. Hauv cov khoom siv hluav taws xob, ib qho me me ntawm tooj liab ntxiv rau kev cuam tshuam qhov tsis zoo ntawm titanium thiab hlau ntawm conductivity. Zirconium lossis titanium tuaj yeem kho cov nplej thiab tswj cov qauv recrystallized. Txhawm rau txhim kho machinability, txhuas thiab bismuth tuaj yeem ntxiv. Hauv Mg2Si, Mg / Si piv yog 1.73. Nyob rau hauv lub tshav kub-kho lub xeev, Mg2Si yaj nyob rau hauv txhuas, muab lub alloy dag dag zog hardening zog. 6061 yuav tsum tau tej yam lub zog, weldability, thiab siab corrosion kuj rau industrial structural Cheebtsam . 6061 yuav tsum muaj ntau yam muaj structural hais nrog tej lub zog, weldability, thiab siab corrosion kuj, xws li cov kav dej, phaj rods siv rau kev tsim kho, ntauwd, thiab ships. rooj tog, machinery qhov chaw, thiab precision machining.

 

Zuag qhia tag nrho, 6061 muaj cov ntsiab lus siab dua ntawm cov ntsiab lus alloying dua 6063, yog li cov khoom siv zog siab dua.

 

Difference between 6063 and 6061 aluminum alloys

 

Xa kev nug

whatsapp

Xov tooj

Tug

Kev nug