Txij li qhov tseem ceeb tshaj plaws ntawm 6082 alloy alloy yog nws muaj cov lus qhia ua kom yooj yim, yog li lub zog tsis txaus, yog li lub zog ua kua los ntawm kev tswj hwm qhov kub ntawm 740 ~ 760 enseny kom ntseeg tau tias cov hlau yog kiag li melted, qhov ntsuas kub yog qhov tseeb thiab muaj pes tsawg leeg nyob rau. Thib ob, Casting yuav tsum txiav txim siab tias cov hlau MN tsub viscosity ntawm alloy, txo nws cov kua qaub, thiab cuam tshuam rau kev ua haujlwm pov thawj ntawm cov alloy. Lub Casting ceev yuav tsum muaj kev txo kom tsim nyog thiab tswj tsis pub dhau ntawm thaj tsam 80 ~ 100mm / min. Qhov thib peb, nce kev siv txias txias thiab ua kom cua txias kom sov, thiab txhuas profiles ua kom tshem tawm cov xwm txheej ntawm kev sib cais. Tswj thawj lub zog txias thiab nce cov txheej txheem sib txawv ntawm theem nrab kom txo cov kev ntxhov siab tsim tawm rau lub sijhawm ua kom pom kev ntxhov siab thiab tsis txhob ingot tawg tsis xws luag. Lub dej txias kom txias yuav tsum tau tswj hwm nyob rau hauv ntau ntawm 0.1 ~ 0.3mpa.
Cov ua rau thiab kev kho ntawm txhuas profile ua zas dye:
1. Tus anodized zaj duab xis tuab yog tsis txaus. Kev daws teeb meem yog tshawb xyuas seb cov txheej txheem anodizing yog cov qauv, thov kho kom haum, thov kho kom haum kom paub tseeb tias cov yeeb yaj kiab tuab ntsib tus qauv.
2. Yog tias tus nqi ntawm tus nqi ntawm cov xim tshaj yog siab dhau, tus nqi PH yuav tuaj yeem hloov kho rau tus qauv txheem nrog glacial acetic acid.
3. Lub workpiece nyob hauv lub dab dej rau ntev dhau tom qab oxidation. Yog tias qhov no tau tshwm sim, qhov ua haujlwm tau muab tso rau hauv anodizing tank lossis nitric acid neutralation tank rau dyeing ua ntej ziab, thiab cov nyhuv yuav ua tau zoo heev.
4. Kev xaiv tsis raug cai ntawm zas xim. Tsim nyog kawg yuav tsum tau xaiv.
5. Qhov xim tau decomposed los yog mildewed, thiab qhov zas yuav tsum tau hloov lub sijhawm no.
6. Cov oxidation kub yog tsawg dhau, uas ua rau muaj yees zaj duab xis. Cov oxidation kub tuaj yeem nce ntxiv.
7. Txom Nyem Kev Ua Haujlwm. Phem tsis zoo yuav raug qhia los ntawm kev tiv tauj tsis zoo ntawm anode tooj liab pas nrig lossis catho do phaj. Them sai sai kom ntxuav cov anode tooj liab pas nrig thiab cathode cov phaj txhuas kom ntseeg tau tias txoj kev ua tau zoo.
Cov pwm ntawm cov hniav radictor muaj ntau cov hniav sib tsoo, txhua tus hniav yuav tsum muaj zog, nws yog qhov yooj yim los ua kom cov hniav tsis muaj zog lossis kev sib tsoo. Yog li ntawd, qhov zoo ntawm pwm hlau yuav tsum tau txhim khu kev qha, thiab nws yog qhov zoo tshaj plaws los siv H13 steel ua los ntawm kev txhim khu kev tsim khoom lag luam, lossis xaiv siab} Zoo} Cov tuab {2} Cov kauj ruam siab txawv teb chaws. Kev kho cua sov ntawm cov pwm tseem ceeb heev, nws yog qhov zoo tshaj plaws kom siv tau cov cua sov quenching, nws tuaj yeem ua kom muaj kev ua tau zoo ntawm txhua qhov ntawm cov pwm tom qab quenching. Tom qab quenching, peb qhov kev npau taws yuav tsum tau noj kom ntseeg tau tias qhov tawv ntawm cov pwm yog lav tau tias yog HRC48 ~ 52, nrog txaus tawv. Nov yog ib qho tseem ceeb rau kev tiv thaiv pwm hniav.