Tus tsim thiab tsim cov nqi ntawm txhuas profile extrusion pwm suav txog li 20% ntawm tag nrho cov nqi tsim khoom. Nws yog ib qho ntawm cov thev naus laus zis tseem ceeb hauv kev lag luam aluminium profile extrusion, uas muaj ntau qhov sib txawv thiab txhim kho sai. Nws koom nrog ntau yam, suav nrog kev xaiv cov khoom siv, tsim, tsim, tshuaj xyuas, kho pwm, thiab kev tswj hwm, thiab tseem yog ib qho ntawm cov cheeb tsam uas muaj peev xwm loj hlob.
1. Ua tib zoo siv cov txheej txheem tsim khoom thiab cov kev cai rau txhuas profiles
Nws yog ib qho tseem ceeb kom nruj me ntsis ua raws li cov txheej txheem txhuas profile extrusion. Thaum lub tshuab pib-nce, qhov kub ntawm qhov nruab nrab ntawm lub tshuab hluav taws xob aluminium yuav tsum tau teem rau ntawm 530-550 degree, thiab qhov hluav taws xob yuav tsum tau teem rau ntawm 480-500℃. Lub sij hawm rwb thaiv tsev yuav tsum txaus los xyuas kom meej tias aluminium billet yog sib npaug rhuab thoob plaws (ob lub hauv paus thiab saum npoo). Qhov no tiv thaiv qhov kub tsis sib xws sab hauv thiab sab nraud ntawm daim tawv nqaij (qhov kub tsis txaus), uas tuaj yeem ua rau elastic deformation ntawm cov tuag, ua rau muaj teeb meem xws li 'tsis sib xws ntawm phab ntsa tuab' thiab 'qhov ntev tsis sib haum,' thiab txawm ua rau cov yas deformation ntawm extrusion tuag, ua rau nws seem.
2. Ua kom 'peb lub siab nyob hauv ib qho'
Lub hauv paus ntawm lub extrusion chim, lub extrusion pas nrig, thiab lub hauv paus tuag yuav tsum visually concentric. Tsis muaj qhov pom tseeb eccentricity raug tso cai, txwv tsis pub nws yuav cuam tshuam tus nqi ntws ntawm ntau qhov chaw ntawm cov khoom, thiab tej zaum yuav cuam tshuam qhov tsim ntawm cov khoom lossis ua rau qhov ntev ntawm ob sab ntawm cov khoom extruded sib txawv, ua rau extrusion ntau lawm ua tsis tau. Rau ntau- qhov pwm uas muaj ntau tshaj li ob qhov tso zis, qhov yuav tsum tau nruj dua.
3. Xaiv cov ntaub ntawv txhawb nqa kom raug
Nws yog ib qho tsim nyog los xaiv qhov tsim nyog qhov loj me ob - qhov, loj cantilever tshwj xeeb kev txhawb nqa pads kom txo qis elastic deformation ntawm cov pwm qis, ua kom ruaj khov extrusion khoom tsim nrog tsawg qhov sib txawv. Ntxiv mus, qhov tshwj xeeb muab ob npaug rau- qhov kev txhawb nqa cov ntaub qhwv yuav tsum tau npaj ua ntej ua ntej cov pwm raug tshem tawm ntawm lub qhov cub, kom tsis txhob txias ntau dhau ntawm cov pwm vim lub sij hawm siv tshawb nrhiav cov ntaub qhwv, uas tuaj yeem ua rau muaj qhov tsis xws luag. Nws kuj tau pom zoo tias cov ntaub qhwv cov ntaub qhwv yuav tsum tau ua kom sov, feem ntau tswj qhov kub ntawm 350 thiab 450 degree. Qhov no yog qhov tseem ceeb tshwj xeeb tshaj yog rau qhov tsis sib xws ntawm cov ntoo khaub lig- ntu thiab ntau- lub qhov, qhov uas nws yog qhov tseem ceeb rau xaiv cov ntaub qhwv tshwj xeeb uas tsim nyog.
4. Txhim kho cov ntaub ntawv tawm tswv yim thaum lub sij hawm txhuas profile extrusion txheej txheem
1) Cov lus teb rau Extrusion Tuag Clogging
Muaj ntau qhov laj thawj rau kev tuag clogging, xws li pwm ua cov teeb meem, cov khoom tau daig hauv cov kab noj hniav khoob, burrs los ntawm cov kab noj hniav khoob, cov kab noj hniav me me, qhov tsis muaj qhov khoob khoob qhov tob, thiab lwm yam cuam tshuam. Tsis tas li ntawd, kev tsim pwm tsim ua haujlwm tsis raug, xws li kev tsim cov dej ntws tsis raug lossis qhov chaw faib khoom, tuaj yeem yooj yim ua rau tuag clogging. Feem ntau, cov neeg uas tsis tau txais kev cob qhia tshwj xeeb yuav pom tias nws nyuaj rau piav qhia qhov no kom meej. Nws yog qhov zoo tshaj plaws rau kev cob qhia cov neeg ua haujlwm kho pwm los tshuaj xyuas cov pwm ntawm tus neeg, txheeb xyuas qhov ua rau, ua pwm txias, kho pwm, thiab tawm tswv yim kev hloov kho.
2) Cov lus teb rau Extrusion khoom tsim
Dhau li kom meej meej kos tus lej extrusion tuag ntawm lub billet, nws kuj tseem yuav tsum tau kos cov kev taw qhia tag nrho ntawm lub billet, uas yuav nyuaj rau pom. Piv txwv li, "converging extrusion" qhia tias nyob rau hauv cov txheej txheem extrusion tiag tiag, sab hauv ntawm ob lub qhov yog qeeb dua thiab sab nraud sai dua; "diverging extrusion" qhia tias sab hauv ntawm ob lub qhov yog nrawm dua thiab sab nraud qeeb dua; "sab laug ntev, txoj cai luv" txhais tau hais tias sab laug ceg ntev thiab ceg sab xis yog luv. Qhov txawv ntawm qhov ntev yuav tsum tau teev tseg. Vim hais tias qhov kev ncua deb ntawm cov saw txiav mus rau lub extrusion tuag qhov hluav taws xob yog kwv yees li 6 meters, nws yog feem ntau sawv cev raws li "A meters / 6 meters," lub ntsiab lus qhov txawv qhov ntev yog A meters ib 6 meters. Xws li cov lus qhia ua tiav thiab raug pab pwm kho cov neeg ua haujlwm txiav txim siab thiab kho kom raug.
3) Cov lus teb rau Dimensional Deviations
Thaum cov khoom extrusion ua ib txwm tab sis qhov sib txawv ntawm qhov sib txawv tshwm sim, nws yog ib qho tseem ceeb uas yuav tsum tau ua cov qauv ntu thiab ua kom tiav thiab raug cov cim (extrusion tuag tooj, extrusion kev taw qhia, qhov tsis xws luag, thiab lwm yam). Txhua qhov cim tsis raug tuaj yeem ua rau kho cov pwm tsis raug, yog li yuav tsum tau ceev faj heev. Kev muab cov qauv coj mus kuaj yog qhov zoo tshaj plaws nrog rau cov ntu ntawm qhov pib, nruab nrab, thiab qhov kawg ntawm daim ntawv billet.